Thread: PP 205. Plasme consumable lifetime question

  1. Default PP 205. Plasme consumable lifetime question

    Hi All...

    I have a PowerPro 205 and just cut some 3/32" sheet aluminum. The settings were 35 Amps and 35 PSI. After 4 feet of cutting it was making wide, messy cuts and the plasma tip hole was opened-up and ragged. I was using the wire nozzle spacer that comes with the torch and was using a guide to cut straight lines. -Nothing fancy. Seems like it wore-out pretty quick. A few questions...

    Is there a chart of recommended settings for various metals and thicknesses?

    When I replace the tip, should the inner electrode be replaced at the same time?

    Are all plasma consumables created the same or are some better than others?

    Thanks...

    Ray
    Last edited by Ray C; 08-13-2012 at 03:11 PM.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Ray C View Post
    The settings were 35 Amps and 35 PSI. After 4 feet of cutting it was making wide, messy cuts and the plasma tip hole was opened-up and ragged. I was using the wire nozzle spacer that comes with the torch and was using a guide to cut straight lines.
    Sounds way too low on the pressure. It depends on the torch you have. Check out the following video for a few tips and settings.

    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    Much thanks! Yep, pressure was too low and it's humid as heck today -and I don't have a dryer on the line... I'll take care of that.

    Ray


    Quote Originally Posted by Rambozo View Post
    Sounds way too low on the pressure. It depends on the torch you have. Check out the following video for a few tips and settings.


  4. Default

    OK, put a dryer in line and put the pressure up to 55 PSI. Everything's peachy now. Works good.

    Thanks again...

  5. #5

    Default

    Quote Originally Posted by Ray C View Post
    OK, put a dryer in line and put the pressure up to 55 PSI. Everything's peachy now. Works good.

    Thanks again...
    Hope the video helped. Glad you are getting the results you need now.

  6. Default

    BTW: The reason I was running at 35 PSI is because that was the recommended level in the instruction manual that came with the unit. The pressure was specified in a range (Pascal units) in which the mid-point converted to 35 PSI.

    Anyhow, I made a welding cart of aluminum this weekend and also did 4 hours of 7018 stick work on 1/2" steel plate. The Power Pro 205 is doing fine but I probably should have got the next bigger model. Much of the AL TIGging this weekend was at 160-180 Amps which is the edge of the machine. I was staying with about a 50% duty cycle and the machine didn't hiccup. I like it. It's a keeper.

  7. #7
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    So what color was the big box where you got that little dryer? I don't ever recall seeing those before.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Ray C View Post
    BTW: The reason I was running at 35 PSI is because that was the recommended level in the instruction manual that came with the unit. The pressure was specified in a range (Pascal units) in which the mid-point converted to 35 PSI.
    From what I understand the manuals shipped with the units are not the best. You can download better ones from the web, here:
    http://www.everlastgenerators.com/manuals.php
    Long arc, short arc, heliarc and in-the-dark!

  9. Default

    Click image for larger version. 

Name:	Dryer.jpg 
Views:	454 
Size:	54.9 KB 
ID:	7627
    Quote Originally Posted by redbeard View Post
    So what color was the big box where you got that little dryer? I don't ever recall seeing those before.
    I got my dryer from a friend who happens to have one he salvaged. It's similar to this one but only had the dryer part. The desicant was saturated and I had to cook it a while in the toaster oven. Now I want to rig-up some valves so I can switch between dry air for plasma machine and normal air for general shop work. I think these things cost about 100 bucks so I'm happy to have got mine free...

  10. #10

    Default

    Quote Originally Posted by redbeard View Post
    So what color was the big box where you got that little dryer? I don't ever recall seeing those before.
    You mean this one? http://www.harborfreight.com/inline-...ter-68215.html

    They work very well for the price, some people bake them back to the blue color. You can actually open them and replace the media too.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  11. #11

    Default

    Yep, Harbor Freight. 8.00. They have/had the replacement silica for it too. Good quality.

  12. #12

    Default

    Great price at $8. Just wonder on quality. Almost everything I have bought from HF has been crap! Bought one of their mig 170's a while back and it worked great the first time I used it, ok the 2nd, and I had to open the unit and turn the wire to weld the 3rd time. I like HF's prices but not their quality. At least returning the crap is easy enough.
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

  13. #13

    Default

    Quote Originally Posted by ShaneJackson View Post
    Great price at $8. Just wonder on quality. Almost everything I have bought from HF has been crap! Bought one of their mig 170's a while back and it worked great the first time I used it, ok the 2nd, and I had to open the unit and turn the wire to weld the 3rd time. I like HF's prices but not their quality. At least returning the crap is easy enough.
    That little water filter works quite well. I have a bunch of them I picked up at $4 on sale.

    Over the years I have learned the good and the bad for me. There are websites with lists on them as well if you google or search here too. They have gotten better over time, the prices also have gone up a little. The old saying I guess (get what you pay for).

    When I buy there I know it is a consumable. Also, the drill bits are a waste. I have a 4.5" grinder that is 8 years old and bought a coleman compressor from them maybe 5 years ago. Weird place for sure, but like you said easy to return something if you made a bad pick.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Consumable factory
    By Titan winch in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 11-02-2013, 12:30 PM
  2. TIG Consumable Lifespan
    By MuttonHawg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-19-2013, 01:54 PM
  3. Stocking Stuffer TIG CONSUMABLE KIT
    By Titan winch in forum Pre-sales, Sales and Shipping questions
    Replies: 15
    Last Post: 02-06-2013, 11:37 AM
  4. Tig Consumable Pricing ??
    By cbmkr in forum Pre-sales, Sales and Shipping questions
    Replies: 2
    Last Post: 07-29-2012, 11:58 AM
  5. consumable question...
    By Brian Ski in forum General Welding Questions
    Replies: 16
    Last Post: 04-14-2012, 12:08 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •