This was a huge bread dough tub i had to make at work,lot of weld then grind then weld and grind some more ,took almost 40 hours.The tub had to be flawless on the inside so no pits good be seen.
This was a huge bread dough tub i had to make at work,lot of weld then grind then weld and grind some more ,took almost 40 hours.The tub had to be flawless on the inside so no pits good be seen.
Last edited by zoama; 08-14-2012 at 12:50 AM. Reason: fix quote tag
so make us all some home made bread lol
EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list
I'm assuming all made with that big old synchro in the background pic?
Miller 210 MIG
Eagle 3-Cylinder Compressor
Air Tools
Body Tools, Shrinker, Stretcher
Bead Blast Cabinet
Homebuilt Car Rotisserie
1971 Dodge Challenger, Pro-Touring, 6.1 Hemi, Fikse Wheels, 335/275 Tires (in progress)
That welder in the background is a aerowave..and the material that was used was 12 ga. coldrolled an it was formed on brake press in 2 halves and the ends added on .
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
nope not stainless ,they power wash them down after each mix and gets completly coated with vegatable oil each time,but i am told i will be making 2 out of stainless.
Where I am, all cooking/eating places are stainless in the back operating parts. Was the project the date/time on the camera or like Ram said, you just need to set it Not that is matters, but I caught that too. I would turn the date stamp off myself.
So it is cold rolled steel, that is surprising for sure. What do you use all the bread for?
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.
Deoderant wasn't the problem, anti perspirant is, with its aluminum active ingredient. I use plain Brut stick deodorant myself,and cap it off with a spray of Brut spray deodorant, just for good measure.
NEVER use an aluminum stock pot to make lime pickles in btw, unless you like watching your pot disintegrate.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
I use Arm & Hammer Essentials Natural Deodorant , has baking soda in it to help from getting rashes when sweating it all natural
EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list
Now this is a turn on a thread that had been about a bread tub! LOL. Holy thread jack batman! Just kidding. It's sort of relevant to the material ..... I think
Miller 210 MIG
Eagle 3-Cylinder Compressor
Air Tools
Body Tools, Shrinker, Stretcher
Bead Blast Cabinet
Homebuilt Car Rotisserie
1971 Dodge Challenger, Pro-Touring, 6.1 Hemi, Fikse Wheels, 335/275 Tires (in progress)
The company i work for made these for another company we are a job shop so i do all kinds of different things,we are not in the buisness of making bread.