    did you unplug peddle and seen if reads ok
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  2. Default

    I am by no means and EE but my PP205 had a display that went in and out and had funny characters showing. I called support and they had me take the cover off and make sure the display connection we tight/secure. It was loose so I secured it and now my display is working fine. I don't know if this will help but, you should call support. Good luck.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  3. #3

    Default

    Any success in figuring out the problem? Of course it is the weekend so I suppose tech support isn't the easiest to get a hold of. Hopefully it is something very simple as suggested by NRM above.
    Miller 210 MIG
    Eagle 3-Cylinder Compressor
    Air Tools
    Body Tools, Shrinker, Stretcher
    Bead Blast Cabinet
    Homebuilt Car Rotisserie

    1971 Dodge Challenger, Pro-Touring, 6.1 Hemi, Fikse Wheels, 335/275 Tires (in progress)

  4. #4
    Join Date
    Jul 2011
    Location
    Southern Middle TN
    Posts
    47

    Default

    Quote Originally Posted by MoparCar View Post
    Any success in figuring out the problem? Of course it is the weekend so I suppose tech support isn't the easiest to get a hold of. Hopefully it is something very simple as suggested by NRM above.

    No luck. I had already tried the things mentioned with out success. I spoke with Ray and he decided the machine needs to be sent back. I hate this as I have to go borrow a tig welder to do some repair and modification work to my dragster. What I dont really understand is it was working flawlessly 6-7 weeks ago and had been sitting in my shop on the cart all rolled up, unplugged nice and tidy in its spot. As soon as I find out what happened Ill let everyone know.
    Everlast Powertig 250EX
    Worlds Quickest Oldsmobile Powered Vehicle
    397 cid Twin Turbocharged Oldsmobile

  5. #5
    Join Date
    Jul 2011
    Location
    Southern Middle TN
    Posts
    47

    Default

    Still waiting on getting this resolved........
    Everlast Powertig 250EX
    Worlds Quickest Oldsmobile Powered Vehicle
    397 cid Twin Turbocharged Oldsmobile

  6. #6
    Join Date
    Jul 2011
    Location
    Southern Middle TN
    Posts
    47

    Default

    I was hoping to have all this behind me by now, just got the machine back Tuesday, box looked alittle rough opened the box UPS has broke the front bezel and pushed back the connections for the ground and torch. Checked to see if anything was grounded out, didnt see anything pulled the panel back out. Put power to the machine, powered up fine, ran for about 30-45 seconds then a loud pop, trips the breaker in the breaker box. Called Ray he instructed me to pull the cover and check the nylon spacers that hold the heat sinks in place all are in place and make sure nothing is shorted or broken. Cannot see any shorts or burnt circuitry or burnt electrical components or burnt smell nothing broken. He said put power back on the machine, powers up fine display OK seems to be working, BUT has no output only the HF . Will not pull any arc when in stick function either. I have become very frustrated at this point Ive been dealing with trying to get my welder back in action for almost 12 wks now. I really really need to get this worked out Im getting really backed up with personal projects along with customer work.
    Everlast Powertig 250EX
    Worlds Quickest Oldsmobile Powered Vehicle
    397 cid Twin Turbocharged Oldsmobile

Similar Threads

  1. 250EX first problem
    By scar1204 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 02-23-2018, 11:20 PM
  2. Replies: 3
    Last Post: 01-22-2016, 03:25 AM
  3. 205 tig problem???
    By braveops in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 01-05-2013, 06:42 PM
  4. Intermittent HF start problem on 250EX
    By vfrguy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 15
    Last Post: 05-06-2011, 12:38 AM
  5. powertig 250ex with water cooler problem
    By DisWeld in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 04-12-2010, 11:29 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •