First project for the contest, just the kind of work I hate to do. Hot, messy, rush job, and missing materials. Oh well, someone has to do it. Needed to fix both skids on a 60" flail mower.

Kinda worn out.
Click image for larger version. 

Name:	Projects 866.JPG 
Views:	1042 
Size:	39.6 KB 
ID:	7462 Click image for larger version. 

Name:	Projects 869.JPG 
Views:	1068 
Size:	60.4 KB 
ID:	7463

Cut a couple of new skids from half inch thick abrasive plate steel.
Click image for larger version. 

Name:	Projects 870.JPG 
Views:	1060 
Size:	63.1 KB 
ID:	7464

Of course the shop is minus a bunch of stuff out on loan, one of which is the torch, so I ended up cutting a groove in them with a cutoff wheel about a quarter inch deep, then bending on the groove and welding the groove shut, instead of heating and bending. Welded them back to the mounting pieces. All with 7018AC and an old Miller Thunderbolt AC buzzbox. It's about the only thing left around here, but it worked fine.
Click image for larger version. 

Name:	Projects 873.JPG 
Views:	1066 
Size:	61.2 KB 
ID:	7465 Click image for larger version. 

Name:	Projects 875.JPG 
Views:	1101 
Size:	59.2 KB 
ID:	7466 Click image for larger version. 

Name:	Projects 876.JPG 
Views:	1099 
Size:	63.2 KB 
ID:	7467

What it had trouble with is the hardfacing I put on the bottom. I was only able to get 5/32 hardfacing rod instead of 1/8 and that little Miller had it's tongue out for that. AC is not the way to go, but it works and I'm hoping this will increase the lifespan. This mower is only about a year old and has not had a lot of use, but plenty of abuse. And of course it has to go out first thing in the morning for a job.
Click image for larger version. 

Name:	Projects 879.JPG 
Views:	1078 
Size:	67.4 KB 
ID:	7468 Click image for larger version. 

Name:	Projects 883.JPG 
Views:	1086 
Size:	41.6 KB 
ID:	7469 Click image for larger version. 

Name:	Projects 884.JPG 
Views:	1120 
Size:	42.4 KB 
ID:	7470