					yes your not steady enough like Rambozo says what help to when i tig i lay the torch lead over my shoulder to balance the weight of the torch instead of lead just  dangling i rest my hang on a old rolled up welding glove to steady my hand when tig welding indexing the torch so your thumb is lined up with torch button will help also. takes time and patience to learn how to tig aluminum you just dont pick up a torch the first time and do welds that are nice looking. also buy some better welding glove designed for tig welding they need to fit snug and easy for finger movement i use these love how they feel when tig welding i use the gloves like your wearing for like stick and mig welding only
 i use these love how they feel when tig welding i use the gloves like your wearing for like stick and mig welding only
				
			 
			
		 
			
			
			
				