I was told I could use torch without water cooler as long as I did not go over 200 so I kept it at 130 and it still melted wtf I guess its time for the weld craft 300 wasn't a big fan of the torch but I only used it a few times but the welder was pretty nice welded just as well as a dynasty 200 I do a lot of field work and dont have time to lug the cooler around with me