Thread: Well I guess it is my turn to learn.

  1. #1

    Default Well I guess it is my turn to learn.

    Just got my 200dx on Tuesday. Got it wired up and all put together this morning. Then I got called away for a couple hours. The quick tip I learned was turn all the knobs to the left and turn the power up. Grabbed a piece of 1/8" and decided to give it a try. I have only seen someone in person once using a TIG. Never even held a torch before.
    Click image for larger version. 

Name:	100_7901.jpg 
Views:	484 
Size:	140.9 KB 
ID:	7414

    Doesn't seem bad for a first time. I am very happy with the machine so far. Welding Aluminum seems to be pretty close to soldering. Lot of things to do and new habits to learn. One problem I found right away. I am used to pulling the torch away... I have to learn to let up on the pedal first. I have been using a MIG for a lot time. Seems strange when done how much heat there is... Maybe still in the back of my mind thinking of soldering.

    I guess I got carried away and tried a lap joint... Thin diamond plate with a bit of a gap in spots... No burn through but having a rough time heating the bottom sheet without burning the top one back. Ah... Learning...

    Click image for larger version. 

Name:	100_7902.jpg 
Views:	462 
Size:	143.7 KB 
ID:	7415
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  2. #2

    Default

    Not bad ... it'll come together ... yea, you can't pull the torch away quickly keep it directly over where you stop w/ post flow. I did it the hard way, for the first two weeks I did everything T2 ... went through $35 worth of gas and $18 worth of filler ... then hooked up the pedal for the first time; what a difference.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

Similar Threads

  1. My 2 year old 211 si won't turn on now
    By conway in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 07-06-2018, 09:22 PM
  2. Can you guess what it will be?
    By jakeru in forum On Road Fabrication
    Replies: 14
    Last Post: 05-15-2012, 05:34 AM
  3. The best rod for the newby to learn on
    By geezer in forum Stick Welding (SMAW)
    Replies: 27
    Last Post: 02-14-2012, 05:28 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •