Brian, it is not coated with copper, but that does not mean it will rust any faster than copper coated wire. I've had copper wire rust on me faster than this stuff. Copper wire will rust. As far as not using it, and the wire rusting, IF a wire does oxidize, it is usually only the top layer of wire, and once that is removed, the wire beneath is just fine, if it is on a closed spool. I live in S. GA, 2 hours from the gulf, and 2 hours from the Atlantic. It doesn't get much more humid, with summer averages around 80-90% humidity.