    i only spray my mig gun not what i am welding
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  2. #42
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    i only spray my mig gun not what i am welding
    Quote Originally Posted by performance View Post
    The only problem with that is that it will cause impurities and porosity in your weld. When that stuff is heated up it goes to gas, and when it does it creates air bubbles beneath the surface of the weld. Only a little should be used inside the gun nozzle and non weld areas.
    I think this is what he was referring to.

    Quote Originally Posted by Rodsmachineshop View Post
    i keep my mig wire from rusting is i spray anti spatter spray on my wire spools i store . . when i get done welding i open my side cover and spray the outside of spool with anti spatter spray works good
    Contaminating the wire with anti-spatter is probably not the best plan. There might be something that would be safe to spray on it, but I don't know what that would be. A lot depends on what you are welding, of course. For general fab it might not be such a big deal, but if you are stressing the weld to near limits or welding something that will be pressurized, it could very well be a big deal.
    Long arc, short arc, heliarc and in-the-dark!

  3. #43

    Default

    I got the wire today. It's sealed in a plastic bag inside the box and the wire itself is in good shape... but. Even though the seller went all out in boxing it to protect the roll, it's been dropped on the round part (like a tire with a flat spot) causing the center hole to be oval now instead of round. It's not too bad, maybe 10% compressed. The sides of the roll are still straight.
    Anyone know how to get the center hole back round without causing more problems ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #44
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by zoama585 View Post
    Anyone know how to get the center hole back round without causing more problems ?
    Something cone shaped?
    Long arc, short arc, heliarc and in-the-dark!

  5. #45

    Default

    I went out to the shop and tapped a 2" pipe into the center of the spool, put a wood block against the 2 bent spokes and knocked them straight, then bumped the outside ring with a rubber hammer and got it to good enough.
    I think it'll feed OK now but I'll have to wait for a cooler day to find out... I'm addicted to A/C and my shop isn't finished yet.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #46

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    i keep my mig wire from rusting is i spray anti spatter spray on my wire spools i store . . when i get done welding i open my side cover and spray the outside of spool with anti spatter spray works good
    Rare we have wire around long enough to rust, but we have the same environment as Mark, actually a little worse. But sometimes a MIG will get ignored like the IMIG200 now that we have the 205P and we will open it and see rust on the wire. Outside of the spool only and we use the copper coated. It does rust.

    We use, I think Eagle brand spray. I think I will try out Rod idea on the 200 and see if it works. Great idea Rod. My brand for sure is not soap. It is a pain to get/clean off even with acetone.

    Also I read Radnor has a water base spray 1630 that is good. Maybe I will give it a try.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. PowerPro 256 makes HF but wont start arc
    By acannell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 06-25-2016, 06:03 AM
  2. What makes PP 60C ideal for CNC?
    By RichardH in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 01-06-2014, 04:25 PM
  3. Powerpro 205 makes me think one day i can call myself a welder
    By Chuck_jkl in forum Customer Testimonials
    Replies: 6
    Last Post: 02-01-2013, 01:05 AM
  4. Replies: 26
    Last Post: 02-22-2012, 11:25 AM
  5. Anyone who makes Aluminum catch cans or reservoirs...Question?
    By CGCINC in forum General Welding Questions
    Replies: 9
    Last Post: 12-08-2011, 01:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •