    Default Best/favorite online source for filler?

    LWS only has 10# packs and wants double the cost of most online places I checked out. $130 for 1/16 309... Weldfabulous wants less than half that, even with shipping it's still a better deal.

    I need to pick up (and add to my list if you think I should)

    308
    309l
    316l (I have lots of surgical steel projects)
    4043
    5356

    In a couple sizes to have on hand. Planning 1# each, I don't have THAT much of most to do, and will buy 10# packs on the next go-round.

    Who is the cheapest/best to deal with?

    Already have ER70S2 in a couple sizes as well as a few spools of MIG laying around.

    I'm going to bite the bullet and just buy stick from Tractor Supply, Lowes and Depot only have one or two sizes and not the rods I want. TSC prices aren't that bad on 7018, 6011, 6013, 6014. around $15 for 10#
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  2. #2

    Default

    I was looking online to find a selection... Alum, 309, ER70S.... Some were great on one or two, but really high on the other. Then I found a pretty good price and selection, then the shipping was like $40... For my first stop I went to the LWS and picked up a selection. From there I will see what I use and what sizes to pick up.

    I know that probably didn't help you much... My experience...
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  3. #3

    Default

    Weldingcity is good for stainless http://www.weldingcity.com/filler-metals-tig/
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    Weldingcity is also a great source for tungsten too I ordered a 10 pk of 2% lanth the price was great and it was shipped out immediately.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  5. #5
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    I bought tungsten from WeldingCity too, best prices I could find. Unfortunately they only stock stainless TIG filler metal. So far the best prices I've found for er70s2 filler has been on eBay, about $35 for a 10# tube with free shipping.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  6. #6
    Join Date
    Feb 2012
    Location
    Indian Shores Beach, FL - U.S.A.
    Posts
    101

    Default

    I purchase all my filler rod at Welding Supply because they have great prices on name brand products.

    WeldingSupply.com
    PowerTig 250EXT ordered on 2/20/12 - AluMig~250P - MasterTig~250AC - Matco Mig~Spot Welder - Giaintec CAT250D - Harris Steelworker Oxy/Acet - Henrob DHC 2000 - Van Norman CB1401 - Lagun FTV1 Mill - CM Mill/Drill - CM 13x40 Lathe - CM 7x12 Bandsaw - CM 6x48 Belt Sander - CM 12 Disc Sander - Baldor 3/4HP Buffer - TP 960 Blast Cab - 48~Box & Pan Break - 52~Foot Shear - 20~Ton Press - 80~Gal 7.5HP Compressor - 9' Snap On Tool Box - 30' Stainless Tool Box Workbench - 3M Speedglas 9100Xx

  7. #7

    Default

    I looked up my old email. It was from USAWELD.com I check on 1 lb of Alum filler, 2lbs of stainless (or vise versa) and 5 lbs of ER70S. The shipping was $50. I asked if they combined shipping and they said place the order and they will see what they can do.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  8. #8

    Default

    htp has good prices on tungsten and filler rod,also got a good deal on 10# er70s for 33.00 from radnor.

  9. #9

    Default

    You can check our Ebay site Dick-Richard is user ID, we currently have some 308 and 316 in 10 lb boxes, We can sell thru Paypal and ship Fedex, I Listed some prices in For Sale on The Forum.
    We get Tungsten from time to time. We currently have approx 300 pounds mixed plasma parts and mig tips nozzles just sitting on the shelf.( There was nothing there for Supercut 50 P or Power Tig 185 Micro at this time)

    You can send a PM to Get a number to call and get more info.

  10. #10
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    I've seen some good prices at WeldingDepot.com, and just ordered some filler metal along with some safety glasses. I like the Jackson Nemesis glasses, and they come in cheater lenses too.

    I was thinking a "Sticky" thread along the lines of "online stores with good prices / good service" might be a good idea. Everybody has their favorites but it's also good to have a backup source, just in case. Just from reading this thread, for instance, there's a lot of alternate sources that I'd never heard of.

    Cyberweld.com has good prices and fast shipping, another choice.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  11. #11
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Just an update, I think I'm set for now... put in an order with weldingsupply.com this morning for some 'on hand' items. Now I have 1/16 and 3/32 lanthanated tungsten, ER70S-2 filler in 1/16 and 3/32, 309 (thanks cbmkr) in 3/32, 308 in 3/32, 4043 and 5356 in 1/16, 3/32, and 1/8. 1LB of each but the 309, figure it's good for a start. Ordered some .030 ER70S-6 for the MIG to go along with the .023 that I seem to have wound up with 3 rolls of. I need some 1/16 in both stainless still as well as 316L, but those will have to wait for next payday as will the 1/8 lanthanated tungsten. Debating on building a small rod oven to keep some 7018 on hand, the 6011 is a PITA, but worked for what I needed.

    I've ordered from Cyberweld and been thrilled, Plenty happy with Weldfabulous, but both places had prices out of line with others on things I needed. We'll see how weldingsupply goes, hopefully smooth, some damn fine prices on filler and tungsten.

    Now, if I can get the shop cleaned between storms this weekend I'll be able to get some welding done. Too much damn wind this week to weld outside anything but stick or flux core.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

Similar Threads

  1. Need an online source for Stainless??
    By CGCINC in forum General Welding Questions
    Replies: 28
    Last Post: 12-26-2011, 11:21 PM
  2. My favorite settings for various cuts, metals and thickness
    By ducksface in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 04-28-2011, 08:27 PM
  3. favorite brand of welding rods.
    By welderdude in forum General Welder Questions
    Replies: 13
    Last Post: 04-27-2011, 12:58 PM
  4. best place online to order filler rod and tourch parts
    By dgarnier in forum General Welder Questions
    Replies: 18
    Last Post: 04-18-2011, 02:36 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •