    I just though I'd throw a propject on the board since I love my 205 so much...
    I used a spool-gun and SS wire and standard shield gas (90-10) although the welds are dark and ugly pentration was great... A lot of the stands are buildt with old bed rails, ths is 316L no paint or rust... The tops of the kegs were cut out with a Jig I made (the first one took about 40 minutes using a dremel, 2"inch cut off and 4" grinder) The first jig cut took about 30 sec using plasma....The kid designed the stand with some sugjestings from me... I think working with metal and working your sons in the garage.... doesn't get any better.... And really now,,,, when they're old enough to enjoy a cigar and some ice cold home brew......

    here's the link....

    http://www.homebrewtalk.com/f51/aces...thread-247512/
    Last edited by zoama; 07-19-2012 at 05:17 PM. Reason: Repaired your link

Similar Threads

  1. HF odds and ends
    By Rambozo in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 0
    Last Post: 03-22-2018, 08:16 AM
  2. 1/0 15' Ground Cable W/Ends and 300 Amp Ground Clamp
    By cbmkr in forum Buy, Sale or Trade
    Replies: 0
    Last Post: 08-22-2012, 06:29 PM
  3. My Welds
    By Oxide00 in forum Other Custom Fabrications
    Replies: 35
    Last Post: 11-09-2011, 11:23 AM
  4. Everlast Canada Moving Sale Ends July 30th
    By Titan winch in forum Everlast Announcements, Contests and Promotions
    Replies: 1
    Last Post: 07-10-2011, 02:10 AM
  5. how are my welds
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 26
    Last Post: 05-20-2011, 01:46 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •