    **Steel rack for my shop**
    I got tired of tripping over steel in the floor so I decided to build a rack to hold it all.....not as easy as I thought it would be. (what is)

    I used a combination of MIG and TIG to complete this job.
    All metal used is 11ga. The uprights are 2" square with a 2" x 4" plate in the front to keep things from rolling off. The basket was made with a mix of 3 1/2" flat, 2" flat, and expanded metal for the bottom.
    I used 4" thinwall pvc for the wall storage.





















    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default







    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3

    Default

    Next is the wall mount for the PVC pipe.




    And my Super Duper Free hand cutting of holes!!! NOT!













    I also needed a way to hold the bottom of the PVC in place and didn't want to go to much trouble so this is what I came up with....

    Last edited by CGCINC; 07-18-2012 at 11:15 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  4. #4

    Default

    Sure another clean shop you really know how to rub it in. Nice work

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Very nice. I like the expanded metal shelves, they can hold small pieces without being crud catchers. From the fastener locations, I'm guessing that they bolt into something more substantial than the sheet metal wall?
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    Quote Originally Posted by Rambozo View Post
    . From the fastener locations, I'm guessing that they bolt into something more substantial than the sheet metal wall?
    Yeah, there are 6x6 posts in the wall. I used 3/8"x 4 1/2" lags. This is probably the most I'll ever have on the rack because I can order metal and have it delivered the next day so there's no reason to sit on a bunch of metal. The stuff I have will be used in my Next project!!!

    Very nice project! You are a project MACHINE. Now I see why you wanted that circle cutter!
    I like making stuff!!!! It doesn't pay well but it's fun


    The reason I left an opening on the left side of the rack is for my Harbor Freight 7x12 band saw!!! Might not get it soon but I Will get it!!
    Last edited by CGCINC; 07-18-2012 at 11:28 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  7. #7
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by CGCINC View Post
    The reason I left an opening on the left side of the rack is for my Harbor Freight 7x12 band saw!!! Might not get it soon but I Will get it!!
    OK, that answered the question I didn't ask!

    I need to rig me up some shelves. Don't have a lot of floor space so going vertical is becoming a necessity.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  8. #8

    Default

    And some pics of it finished...













    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  9. #9
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Very nice project! You are a project MACHINE. Now I see why you wanted that circle cutter!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  10. #10

    Default

    Very nice ... well thought out!
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  11. #11

    Default

    Quote Originally Posted by Winky View Post
    Very nice ... well thought out!
    I double what winky says. Something I need to do when I get some time. Right now they just lean against the ceiling joists.

    ken
    UNT 520D plasma/stick/tig; Hobart Handler 140 Mig; HF 80amp stick welder; Victor O/A; 4x6 Horizontal bandsaw; Planishing hammer; & Stuff

  12. #12

    Default

    This made a Huge difference!! Everything is up and out of the way AND, I can put my small stuff in the baskets so it free's up part of a closet!
    Was well worth the 5lbs. of sweat and burn't thumb!!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  13. #13

    Default

    Looks really nice... Reminds me of the story of the guy who buys a wallet so he will have a place for his money... Then he has no money to put in the wallet...

    BTW If you have to much metal and you are tripping over it... I will send you my address....
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

Similar Threads

  1. Replies: 59
    Last Post: 02-19-2013, 10:16 AM
  2. Replies: 12
    Last Post: 12-30-2012, 05:05 PM
  3. Replies: 28
    Last Post: 12-26-2012, 02:01 AM
  4. Replies: 7
    Last Post: 10-15-2012, 05:06 PM
  5. Replies: 18
    Last Post: 09-07-2012, 06:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •