    Hi
    Ive had my unit for almost 2 years now. Ive had a couple minor Issues with it but managed to figure them out on my own but Im stumped with this one.

    I went to use my plasma today and it would'nt light the pilot arc I tried everything I could think of (air pressure ground checked the torch leads and even took the torch apart to check the continuity of the wires going from the torch to the machine it all checked out good. The air solenoid does click on when the trigger is pressed . I also hooked up the tig torch and it wouldnt work unless it was scratch started.

    I hope it hasn't crapped out on me I dont feel like spending money on shipping it out to get fixed.

  2. #2

    Default

    Quote Originally Posted by joop View Post
    Hi
    Ive had my unit for almost 2 years now. Ive had a couple minor Issues with it but managed to figure them out on my own but Im stumped with this one.

    I went to use my plasma today and it would'nt light the pilot arc I tried everything I could think of (air pressure ground checked the torch leads and even took the torch apart to check the continuity of the wires going from the torch to the machine it all checked out good. The air solenoid does click on when the trigger is pressed . I also hooked up the tig torch and it wouldnt work unless it was scratch started.

    I hope it hasn't crapped out on me I dont feel like spending money on shipping it out to get fixed.
    It's an easy fix. You need to adjust the HF points in the front of your machine. Here's a thread with some good info http://www.everlastgenerators.com/fo...=adjust+points If you need more help just call the tech line.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    Quote Originally Posted by zoama585 View Post
    It's an easy fix. You need to adjust the HF points in the front of your machine. Here's a thread with some good info http://www.everlastgenerators.com/fo...=adjust+points If you need more help just call the tech line.
    Was thinking the same thing... I guess they can get bumped out of position easy... Let us know if it works for you. I always like to know what fixes things.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  4. #4
    Join Date
    Dec 2010
    Location
    North Bay, Ontario
    Posts
    9

    Default

    Ok Ill try that out.

    I dont really see how that would be the problem as it has worked for almost 2 years without a hitch. The contact points dont look flimsy enough to move on their own but who knows Ill check it out.

    I also forget to add in the first thread its a PP256.

    Could the hf points get dirty and stop arcing across?
    or get dirty and create alot of current trying to jump the arc and overheat the circuit and fry something?

    Now that I think about it these welders would make a perfect detonator in the wrong conditions in a garage. The HF start is basically a spark plug. I guess ill have to thing of that when using flammable liquids around the machine.

  5. #5
    Join Date
    Dec 2010
    Location
    North Bay, Ontario
    Posts
    9

    Default

    Well I feel pretty dumb now hahah.

    Its been 10 min since my last post and I found out the problem.

    I guess I must have bumped the pre-flow up a bit because I turned it down and voila the hf kicks in. DOH!!!!!

    Well at least this thread will be around to help any other absent minded individuals in the future.

    Thanks guys for the links It made it a fast fix. or should I say fast adjustment lol.

  6. #6

    Default

    Well I am glad it was something simple. From what I have heard the points can get dirty or something caught in them to short them.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  7. Default

    Joop don’t feel bad I did something similar. I have the PP205 and it works great, but about 4 months ago the arc would not break when I had the foot pedal back (off position). I checked everything, argon, connections, tungsten, ground, pedal, torch switch. So I called Ray told him what was going on and he said to check the end amps and I ASSURED him they were set to 0, but I would check. Sure enough the end amps was turned up a bit and when set back to 0 everything worked just fine.

    Another one was the HF would not start after the second month of owning my unit, worked fine before. Again checked everything like I listed before and nothing. I turned the amps way up and nothing except one time the arc blasted out and scared the heck out of me. So after looking at all the settings for about an hour and a half I realized I did not turn on the argon. Turned it on and everything was just fine. I felt like such an idiot, but unfortunately that is how I learn most of the time.

    I’m glad to hear you are up and running again.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  8. #8

    Default

    Quote Originally Posted by joop View Post
    Well I feel pretty dumb now hahah.
    So, I had a post all ready to go about my plasma cutter not working. I was certain that I had everything setup right, had pictures to prove it. Just looked at the pictures one last time before I hit the post button, and realized I had the torch in "+" . You shouldn't feel bad at all .... we're all pretty dumb.

    Cheers
    Mike
    Power Pro 256

  9. #9
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by joop View Post
    Now that I think about it these welders would make a perfect detonator in the wrong conditions in a garage. The HF start is basically a spark plug. I guess ill have to thing of that when using flammable liquids around the machine.
    And that would make the welding or cutting arc a blasting cap?
    Long arc, short arc, heliarc and in-the-dark!

  10. #10
    Join Date
    Dec 2010
    Location
    North Bay, Ontario
    Posts
    9

    Default

    hahah ya I guess so

Similar Threads

  1. Pilot arc stability
    By Tallguy64 in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 01-06-2016, 03:19 AM
  2. PO 256 pilot arc ooooops
    By tnc110 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 0
    Last Post: 10-12-2014, 10:04 PM
  3. No Pilot Arc with PP256
    By deepsnow in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 05-30-2014, 07:43 PM
  4. HF start or Pilot Arc
    By Odyknuck in forum Everlast Plasma Cutters (PAC)
    Replies: 12
    Last Post: 09-19-2012, 02:01 AM
  5. intermit pilot arc with CT520
    By cardoc in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 10
    Last Post: 01-20-2011, 12:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •