    This was going to have a little welding in it, but I changed my mind. I was going to make it out of half inch and build up the top part with weld, but in the end I just whittled it out of 3/4 stock, instead. These are mounts to attach some areo bars to a pair of bicycles.

    Started with 3/4" x 2" 6061 T-6 extruded bar.

    Click image for larger version. 

Name:	Bike 001.JPG 
Views:	618 
Size:	57.3 KB 
ID:	7302

    Carve out one side.

    Click image for larger version. 

Name:	Bike 002.JPG 
Views:	619 
Size:	76.8 KB 
ID:	7303

    Flip it and do the other side. Bore the holes and profile the part out.

    Click image for larger version. 

Name:	Bike 003.JPG 
Views:	635 
Size:	50.0 KB 
ID:	7304Click image for larger version. 

Name:	Bike 004.JPG 
Views:	617 
Size:	52.0 KB 
ID:	7305

    Flip again and drill, tap, clearance, and counterbore a couple of holes. Profile the ends round.

    Click image for larger version. 

Name:	Bike 005.JPG 
Views:	633 
Size:	47.7 KB 
ID:	7306

    Flip and scoop out the top. Drill and tap a hole.

    Click image for larger version. 

Name:	Bike 006.JPG 
Views:	648 
Size:	60.7 KB 
ID:	7307

    Here they are mounted to the bars.

    Click image for larger version. 

Name:	Bike 007.JPG 
Views:	620 
Size:	33.4 KB 
ID:	7308Click image for larger version. 

Name:	Bike 008.JPG 
Views:	619 
Size:	80.1 KB 
ID:	7309

    Test fitted on some handlebar tubing.

    Click image for larger version. 

Name:	Bike 009.JPG 
Views:	634 
Size:	46.7 KB 
ID:	7310Click image for larger version. 

Name:	Bike 010.JPG 
Views:	629 
Size:	46.3 KB 
ID:	7311

    I'll probably give them a nice glass bead blasted finish to smooth out the machining marks. Although first I have to clear some junk away from the bead blast cabinet, and I think fix some air fittings on it. Shop maintenance never ends.
    Long arc, short arc, heliarc and in-the-dark!

  2. #2
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Nice pieces! Should look even sharper with the blasting done. Thanks for the pics.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  3. #3

    Default

    or put in a tumbler and polish
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  4. #4

    Default

    Nice work... I like projects with machining.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Nicely done- are you the cyclist? My list of future toys includes "lathe" and "mill" but projects like this move "mill" closer to the top of the list. Do you mind describing your setup?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by DaveO View Post
    Nicely done- are you the cyclist? My list of future toys includes "lathe" and "mill" but projects like this move "mill" closer to the top of the list. Do you mind describing your setup?
    They are for my fiancé and I. A lathe is usually the first machine tool, but these days the line between mill and lathe gets blurry. These parts could have been made on either, but I used a mill. Specifically an old Alliant 42VC 2HP varispeed with an Anilam CNC control circa mid 1980's. Due to space issues I had to get rid of my big lathe, so now I have an import 9x20 that does the job. Space is one of the big reasons I'm looking to replace my TIG machine with an Everlast.
    Long arc, short arc, heliarc and in-the-dark!

  7. Default

    Very nice and clean looking. Did you calculate the weight?
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by NRM View Post
    Very nice and clean looking. Did you calculate the weight?
    Nope, I just used a 2D program to draw them out, so no volume calculations. I did try to keep them pretty light, but nothing extreme. They came out to just over 40 grams each, and with stainless hardware just over 60 grams. Actually, until you asked, I didn't even bother to weigh them.
    Long arc, short arc, heliarc and in-the-dark!

  9. #9
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Very nice. Those machined patterns sure look purdy. That's some pretty thick bar stock you started out with. My wife has been getting me into road biking as well lately. A fun and healthy activity to do together for sure.
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. 4bt Cummins motor mounts
    By dzljon in forum Other Custom Fabrications
    Replies: 12
    Last Post: 08-31-2016, 06:14 AM
  2. Anti-roll bar link mounts
    By its_34 in forum On Road Fabrication
    Replies: 5
    Last Post: 08-17-2013, 04:42 AM
  3. Project 5 Mean Green Contest, SeanMurphy265, Mobile Home Leaf Spring Mounts
    By SeanMurphy265 in forum Heavy Equipment and Commercial Projects
    Replies: 3
    Last Post: 05-23-2012, 01:26 AM
  4. Shackle mounts
    By roadymi in forum Off Road Fabrication
    Replies: 4
    Last Post: 09-24-2009, 12:48 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •