Quote Originally Posted by Rodsmachineshop View Post
yes but would recommend the IGBT instead of Toshiba/Fuji Mosfet that you posted night and day differences on cutting
I'm looking at the difference... $200 more for IGBT. And the cheaper one would do what I want.....I think!?!