  1. Default Welding: Rod-to-Rod Jig

    I got this rod to rod jig idea off another site and thought it was pretty good. My jig is made of 1” aluminum angle (because that is what I had), the window is 2” long and the total length is 4” long. I had a couple of short SS 3/8” rods lying around and did not want to cut a larger piece down. I beveled the ends to be welded on the lathe, clamped them in the jig, welded them together and finished the rod off on the lathe.
    Pic 1 &2 – Two pieces beveled and clamped in the jig (top and bottom view).
    Click image for larger version. 

Name:	Rod to Rod 1.jpg 
Views:	624 
Size:	130.4 KB 
ID:	7205Click image for larger version. 

Name:	Rod to Rod 2.jpg 
Views:	647 
Size:	133.2 KB 
ID:	7206
    Pic 3 – Welded pieces after wire brushing.
    Click image for larger version. 

Name:	Rod to Rod 3.jpg 
Views:	614 
Size:	130.4 KB 
ID:	7207
    Pic 4 – Finished rod, just a couple of pits I didn’t fill in.
    Click image for larger version. 

Name:	Rod to Rod 4.jpg 
Views:	647 
Size:	124.8 KB 
ID:	7208

    It was a very easy to align the rods and the final produce spun pretty true in the lathe.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  2. #2

    Default

    I like it!! Thanks for posting it, I like gadgets!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3

    Default

    That's one I have used for years, for welding up axles for trailers square and other things. It works for square tubing or almost anything for holding and aligning correctly

Similar Threads

  1. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •