    Default Project 1.325 CGCINC: Simple Pull-up bar

    I was bored so I decided to make me a lat pull-up bar.
    I have one similar but my wife and I have to take turns when we do our P90x so this will solve the problem.

    Nothing high tech, just 1" tubing (1/8" wall) cut at an angle, bent together and welded.
    Then some 3/8" plate for the mounts, black paint, and some padded rubber handles and it's done!

    Cut.....


    Bend.....


    Tack.....


    OR... Tack and show off the best purchase Ever!!! My Mojo Viking helmet!!


    Weld and grind tubing.....






    Weld brackets on....


    Close-up....
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    Paint....


    Rubber handle....



    Done!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Nice! I like how the weld on the bend cleaned up really well. what did you use for the foam handles?
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by undercut View Post
    Nice! I like how the weld on the bend cleaned up really well. what did you use for the foam handles?
    Looks like bicycle handlebar grip, to me.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by undercut View Post
    Nice! I like how the weld on the bend cleaned up really well. what did you use for the foam handles?
    No doubt. That is about the nicest grinding job I have ever seen.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  6. #6
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by redbeard View Post
    No doubt. That is about the nicest grinding job I have ever seen.
    You've got that right. No bumps, no crevices or inclusions. Too bad it was covered up with the foam and paint! Mind you, only a welder would really appreciate that it was originally two bars welded together. Everyone else might just roll their eyes. LOL.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  7. Default

    2x on the grinding, great work.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  8. #8

    Default

    Quote Originally Posted by undercut View Post
    Nice! I like how the weld on the bend cleaned up really well. what did you use for the foam handles?
    I bought the rubber handle covers from a fitness equipment supplier online. They come in many different lengths.
    I actually ground the welds smooth because I planned on putting one mount in the middle and sliding longer handle covers all the way to the mount.
    After thinking about it, I figured two mounts would be better at stopping the swaying motion.

    Thanks all! .... Now, when I win some Green bucks and get my plasma cutter, your gonna see some crazy stuff!!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  9. #9

    Default

    Quote Originally Posted by redbeard View Post
    No doubt. That is about the nicest grinding job I have ever seen.
    I am following the rest of the crew... Really nice job... I really hated to see paint put on top of it.... That is a nice weld and cleanup...
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  10. #10

    Default

    Quote Originally Posted by undercut View Post
    Mind you, only a welder would really appreciate that it was originally two bars welded together. Everyone else might just roll their eyes. LOL.
    I was thinking the same thing... I am doing some concrete work. I put a approach on the garage door and a patio/porch on the back of the house. Now I am working on the drive. Lot of work on the prep... Getting the slopes right... When ever you go anywhere you look at the concrete and see what was done... One thing I have noticed is that the concrete break lines need to be 1/4 of the thickness of the slab... They very seldom are... And they very often crack... NOT on the break lines... Way to shallow. I have seen break lines about a 1/4" and that is from the "pros". Boy did I get off topic here....
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  11. #11

    Default

    concrete is easy my dad did it and brick laying trick in concrete is wetting and not being in a hurry
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  12. #12

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    concrete is easy
    Swwweeeeeet.... So when are you stopping by??? We can set the forms and knock out a couple pours!!!!!

    Ya ya... Get started and don't wait for you...... Have heard it all before...
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  13. #13
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by CGCINC View Post
    Now, when I win some Green bucks and get my plasma cutter, your gonna see some crazy stuff!!
    Good choice of equipment for your winnings! Can't wait to see the projects.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  14. #14
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Brian Ski View Post
    I was thinking the same thing... I am doing some concrete work. I put a approach on the garage door and a patio/porch on the back of the house. Now I am working on the drive. Lot of work on the prep... Getting the slopes right... When ever you go anywhere you look at the concrete and see what was done... One thing I have noticed is that the concrete break lines need to be 1/4 of the thickness of the slab... They very seldom are... And they very often crack... NOT on the break lines... Way to shallow. I have seen break lines about a 1/4" and that is from the "pros". Boy did I get off topic here....
    I think it all goes to show that in today's day and age, it seems like only the craftsman still appreciates craftsmanship.

    As for the concrete break lines, sometimes I think they guy who did it thought the lines are there for looks only!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

Similar Threads

  1. Replies: 31
    Last Post: 10-25-2013, 05:27 AM
  2. Project 1 from CGCINC. Category: Welding Cart
    By CGCINC in forum Other Custom Fabrications
    Replies: 20
    Last Post: 11-30-2012, 09:05 PM
  3. Simple but great 250EXT modification/project - With a bonus!!!
    By todmorg in forum Other Custom Fabrications
    Replies: 8
    Last Post: 04-27-2012, 11:37 PM
  4. CGCINC Project#5: Weight Stand
    By CGCINC in forum Hobyist Projects
    Replies: 8
    Last Post: 12-17-2011, 06:45 PM
  5. CGCINC Project#2: TIG filler rod holders
    By CGCINC in forum Hobyist Projects
    Replies: 9
    Last Post: 12-09-2011, 08:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •