    Well, one of my relatives broke their folding chair. Not terribly expensive chair at that. Good opportunity for to make some sparks and attempt a weld. Sorry, I forgot to take the "before" pictures.

    Special Challenges - The tubing that was used was pretty thin. The original welds weren't much more than tack welds, one on each side of tubing for the leg rest that attached to the legs of the chair. Also, I had yet to discover that the Harbor Freight 80 amp inverter welder that I had recently bought was defective!

    Process - SMAW - used 6013 1/16 at "some amperage". Apparently the amperage control was the first to exhibit problems. Turning the knob one way or the other didn't seem to do much. Blew a few holes right off the bat. Managed to move fast enough to repair the holes and eventually welded the tubes together but then the welder went very, very cold and left pock marks and stuck when I was getting near the end. Ground down the rough spots.

    Materials Used - Nothing other than the tubing from the chair and the electrode.

    Sorry this one wasn't exciting .... Was hoping it would be a good starter project to practice on. Returned the Harbor Freight welder. Want a new welder!

    Click image for larger version. 

Name:	20120612_191616.jpg 
Views:	533 
Size:	13.9 KB 
ID:	7125Click image for larger version. 

Name:	20120612_191631.jpg 
Views:	537 
Size:	17.7 KB 
ID:	7126Click image for larger version. 

Name:	20120612_191659.jpg 
Views:	498 
Size:	17.5 KB 
ID:	7127Click image for larger version. 

Name:	20120612_191726.jpg 
Views:	512 
Size:	16.0 KB 
ID:	7128

    Final outcome (before painting).

    Click image for larger version. 

Name:	20120612_191559.jpg 
Views:	521 
Size:	19.7 KB 
ID:	7124
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  2. #2

    Default

    Not knowing where your at with amperage Might be a problem!

    At least you overcame your troubles and Succeeded!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by CGCINC View Post
    Not knowing where your at with amperage Might be a problem!

    At least you overcame your troubles and Succeeded!
    Hey, thanks! The chair was on its last legs (pun intended!) so it was a good guinea pig. Was not a good introduction to welding. Near the end, the arc would sputter and there were pock marks everywhere as I tried to finish the thing off.

    After a long hiatus, I will once again start the learning curve of "watch the puddle, not the arc". So much easier reading than doing!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  4. #4

    Default

    Quote Originally Posted by undercut View Post
    Is it OK to want to break something just so that you can weld it back together?
    Ah so now we know how the chair got broke!!!!!

    Got a couple cheap chairs here... They are brand new... One fell apart like yours and another the spot welds for the backrest came loose.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  5. #5
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Brian Ski View Post
    Ah so now we know how the chair got broke!!!!!

    Got a couple cheap chairs here... They are brand new... One fell apart like yours and another the spot welds for the backrest came loose.
    Someone in the forum suggested that I get a plasma cutter. Then I can cut things apart and put them back together again forever! Hope I don't offend that person because I forgot who exactly it was ... but it sure made me laugh!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

Similar Threads

  1. Project 2 from Youngnstudly. Category: General Welding Repair
    By youngnstudly in forum Welding Repairs
    Replies: 7
    Last Post: 02-01-2013, 05:34 AM
  2. Project 4 from Trip. Category: General Welding repair
    By Trip59 in forum Welding Repairs
    Replies: 20
    Last Post: 01-23-2013, 04:15 AM
  3. Project 2 from ShaneJackson. Category: General Welding repair
    By ShaneJackson in forum Welding Repairs
    Replies: 5
    Last Post: 09-01-2012, 06:15 PM
  4. Project 1 from Rambozo. Category: General Welding repair
    By Rambozo in forum Heavy Equipment and Commercial Projects
    Replies: 14
    Last Post: 08-01-2012, 12:45 AM
  5. Project 1 from CGCINC: Category: General welding repair
    By CGCINC in forum Welding Repairs
    Replies: 15
    Last Post: 07-17-2012, 02:24 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •