Wire size question...?
		
		
				
				
		
			
				
					I've been using my IMIG200 with .030 wire in it, 2lb. spools.   I'm almost out of my last 2lb. .030 wire and I have an 11lb. roll of .035.  
The .030 wire is all I've used in this welder so this is why I'm asking about the .035. 
I weld thinner material, 1/16", 1/8"..maybe 3/16"... Will the .035 wire be ok to run or should I save it and go get some .030?
I just don't want to load an 11lb. spool and then have to take it out mid roll if it doesn't work for me...
				
			 
			
		 
			
				
			
			
				PowerTig 250EX
Power I-MIG 200
Power Plasma 50
It's what you learn, After you know it all, that counts!