    Just received this in my email, and I thought I'd share.

    Comparing Tig Settings using Miller Dynasty 200dx, Lincoln Invertec v205t, and Everlast 210 ext

    Why are some of the controls so different? For example, why is the AC Balance of -15 actually a 65?

  2. #2

    Default

    Because "balance" is 50/50. S/F....Ken M
    Lincoln Power MIG 300
    Everlast 160STH
    Miller 225 Thunderbolt (sold it)
    Lincoln Squarewave 175 TIG(traded it for)
    Miller DEL 200 welder/genset
    Thermal Dynamics 1250XL plasma cutter
    Miller XMT300

  3. #3

    Default

    Balance at 50/50 is set at 0. This is not a thing unique to us btw...just not in the two most popular brands.

  4. #4

    Default

    OK, we are talking alternating current. A percent plus and minus of 0 or center line.

    Their way, think of 50% as in the middle (50% plus of 0 and 50% minus of zero as the wave goes up and down). We call that a 0% offset on our panel, so 50% positive and 50% negative from 0.

    0 with our unit is even amount of + and - (50% plus and 50% minus, in the middle to them is 50. we call that 0).

    So more negative cleaning or positive in our case is from from 0 crossing line. Now go "negative" 15% from 0 on ours display would be -15 for us, or 65% (15% more negative of 50% or 65%) cleaning.

    Hope that helps, but the balance has always been something Miller worded wrong from the start and some others copied.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    OK. That makes sense.

    The little Inverter I have now doesn't have any settings. It is either ON or OFF. All those settings seem overwhelming, but I am sure they help produce a much better weld.

  6. #6

    Default

    Quote Originally Posted by jp2code View Post
    All those settings seem overwhelming, but I am sure they help produce a much better weld.
    I think the operator is the most important part. All the fancy settings in the world don't make up for welder skill... They are neat though :-)
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. Everlast 255EXT and 210EXT Review w/Video
    By christian in forum Customer Testimonials
    Replies: 0
    Last Post: 12-14-2017, 07:59 PM
  2. Video review of PowerArc 160 STH TIG
    By youngnstudly in forum Customer Testimonials
    Replies: 14
    Last Post: 07-09-2014, 07:02 AM
  3. Video Review Stick Welding With PowerTig 200 DX
    By cbmkr in forum Stick Welding (SMAW)
    Replies: 7
    Last Post: 02-28-2013, 01:41 AM
  4. video review of the 200DX
    By Winky in forum Customer Testimonials
    Replies: 27
    Last Post: 10-03-2012, 12:58 PM
  5. Everlast 160 STH Video Review
    By jp2code in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 07-03-2012, 09:04 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •