    This could kind of be looked at like the duty cycle right? I have had it explained to me that with a 60% duty cycle, you need to let it cool for 40% of the time, so, if you weld solid for 6 minutes, let it cool for 4 minutes. Never hurts to go over that though I am sure.
    http://www.facebook.com/CBRMetalworks

    '96 Tacoma V6 on 37's, full custom, built for racin!
    Yamaha Rhino w/ 800 Rotax built for racin!
    Miller 251 MIG
    Everlast Powerplasma 60C with CNC plasma table

    Looking for sponsors for KOH 2013 race!
    Racin' Tacoma Build Thread

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Tacoma747 View Post
    This could kind of be looked at like the duty cycle right? I have had it explained to me that with a 60% duty cycle, you need to let it cool for 40% of the time, so, if you weld solid for 6 minutes, let it cool for 4 minutes. Never hurts to go over that though I am sure.
    Duty cycle is typically measured in 10 minute blocks, so you have it exactly right. Max weld time is 6 minutes with a 4 minute cool down in any 10 minute period. For example 3 on, 2 off, 3 on, 2 off, etc...
    If you go over the duty cycle it is not good on the equipment. Even with protection devices, it's never good to trip them on a regular basis.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Rambozo View Post
    Duty cycle is typically measured in 10 minute blocks, so you have it exactly right. Max weld time is 6 minutes with a 4 minute cool down in any 10 minute period. For example 3 on, 2 off, 3 on, 2 off, etc...
    If you go over the duty cycle it is not good on the equipment. Even with protection devices, it's never good to trip them on a regular basis.
    The 10 minute period is important. Going 12 minutes on and 8 minutes off for a 60% duty cycle is NOT cool. (Pun not intended!)
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  4. #4

    Default

    Quote Originally Posted by undercut View Post
    The 10 minute period is important. Going 12 minutes on and 8 minutes off for a 60% duty cycle is NOT cool. (Pun not intended!)
    You guys must be pros... I can't weld straight through... I am always stopping and repositioning parts. Cleaning them up and continuing the bead.

    I never thought of a cool down time, but I usually don't run the machine that hard. If I run up the power it is not for a very long time, just short bursts. From what I remember I don't think I have ever tripped the thermal cutout.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  5. #5
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    No-one really does. That's why welders have duty cycles. In theory my LX225 can't weld at 225 straight for 24 hours, but in practice I'm only actually welding half the time (or much less!) If I were a robot welding pipe seams or something like that, well that would be different.

    The only time I managed to get a temperature cut out was because I forgot to connect the temperature sensor!

  6. #6

    Default

    Duty cycle probably only really comes into play with either really small welders (and people overusing them), or in manufacturing work where they are being used constantly with little downtime.
    http://www.facebook.com/CBRMetalworks

    '96 Tacoma V6 on 37's, full custom, built for racin!
    Yamaha Rhino w/ 800 Rotax built for racin!
    Miller 251 MIG
    Everlast Powerplasma 60C with CNC plasma table

    Looking for sponsors for KOH 2013 race!
    Racin' Tacoma Build Thread

Similar Threads

  1. This would be cool
    By dzljon in forum Metal Art
    Replies: 1
    Last Post: 01-05-2015, 10:52 PM
  2. cool down/duty cycle
    By ogre in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 12-19-2013, 05:07 PM
  3. sorta cool
    By Rodsmachineshop in forum Everlast Plasma Cutters (PAC)
    Replies: 14
    Last Post: 05-17-2012, 05:30 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •