Share
Results 1 to 16 of 16

Thread: Cool down?

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Cool down?

    I just purchased an everlasting 250ex. Is it ok to power off after welding, or is there a certain amount of time I should leave it on with the fan running?

  2. #2

    Default

    if its hot outside i leave my 250 run for a few minutes after welding
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #3
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Personally, I would. I try to keep my electronics as cool as possible and if I can spare the couple of minutes to allow the fan to run, I do it.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  4. #4

    Default

    I'd call it 10 minutes to be on the safe side.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. Default

    Like Zoama said 10 minutes. I leave my PP205 on while I clean up and it's turned off right before I put it away.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  6. #6

    Default

    I always leave anything with a fan that cuts on/off based on temperature on until the fan shuts off (my MIG welder), my plasma cutter I just let it run for a few minutes after I am done with it, unless I only used it for a very short period. I always leave it on until the air solenoid shuts off air to the torch at a minimum, normally a few minutes longer.

    My MIG welder does not have a fan running at all once the cooling fan shuts off, so I shouldn't have any worries with it.
    http://www.facebook.com/CBRMetalworks

    '96 Tacoma V6 on 37's, full custom, built for racin!
    Yamaha Rhino w/ 800 Rotax built for racin!
    Miller 251 MIG
    Everlast Powerplasma 60C with CNC plasma table

    Looking for sponsors for KOH 2013 race!
    Racin' Tacoma Build Thread

  7. Default

    I usually base the time I let it run on what I have been doing with the welder. A quick tack or two and I will let it sit for 10-15 seconds and shut it off. If I have been blasting away on some heavy aluminum I might let it run for 5-10 minutes.
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

Similar Threads

  1. This would be cool
    By dzljon in forum Metal Art
    Replies: 1
    Last Post: 01-05-2015, 11:52 PM
  2. cool down/duty cycle
    By ogre in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 12-19-2013, 06:07 PM
  3. sorta cool
    By Rodsmachineshop in forum Everlast Plasma Cutters (PAC)
    Replies: 14
    Last Post: 05-17-2012, 06:30 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •