CGC I probably didn’t get good penetration everywhere but my scale goes to 440lbs and big ahi (yellow fin tuna) around here weigh 180-250lbs so I think I will be safe. If we catch a marlin then that will go on the scales at the dock. If I had to do it again I would make a mock setup with PVC to get the coping right. The angle in line with the top tube was easy it was the angle perpendicular to the top tube that was a disaster. Also I would weld the entire thing using tig not stick.