  1. #10
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by posixPilot View Post
    I have a couple of these, and they are fine as long as you thread the top on squarely. Northern has an identical one, but the want like $15 for it.
    You know, I keep seeing those, look at them for a bit and keep walking because I don't know if they are any good and figure that surely I have something at home that would do. Nice to hear from someone who's used them because I still haven't found anything at home that would do better and need to buy some rods soon.

    Just read the reviews on this rod holder. One person says they only hold 5 pounds of rods. I thought they were bigger than that(?)

    Thanks for feedback on this.
    Last edited by undercut; 06-09-2012 at 03:00 AM.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

Similar Threads

  1. Free welding rods... help?
    By CGCINC in forum Stick Welding (SMAW)
    Replies: 17
    Last Post: 06-05-2012, 04:08 PM
  2. Small welding rods
    By Jules The Great in forum Stick Welding (SMAW)
    Replies: 9
    Last Post: 04-23-2012, 12:01 PM
  3. buy dinse conectors and welding rods
    By bobwills in forum General Welding Questions
    Replies: 8
    Last Post: 12-13-2011, 12:52 AM
  4. Don't use gas welding rods for tig
    By Steve in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 10-10-2011, 05:05 AM
  5. favorite brand of welding rods.
    By welderdude in forum General Welder Questions
    Replies: 13
    Last Post: 04-27-2011, 12:58 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •