Share
Page 1 of 2 12 LastLast
Results 1 to 20 of 57

Thread: tungsten choice

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default tungsten choice

    Been welding for about a decade but I am a noob when it comes to AC TIG welding ... in anticipation of the arrival of my new machine I stopped at Airgas yesterday grabbed some aluminum filler rod and asked the guy behind the counter for some 2% lanthinated tungsten ... he sees I have aluminum and tells me the lanthinated is for steel and stainless only ... I asked him what I should be using and he says pure tungsten. Now this guy has never steered me wrong before but I've heard from many people that pure tungsten is pure crap ... I think I even heard Jody say to stay with the 2% ... so now I'm totally confused.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  2. #2

    Default

    he needs to get with the times , pure is for tig old machines but not on the new ones . 2% lanthinated tungsten or Tungsten, 2% Ceriated, is the rite for the everlast machine . not pure . the manual say do not use pure tungsten http://www.everlastgenerators.com/do...ertigfinal.pdf
    Last edited by Rodsmachineshop; 06-07-2012 at 05:32 PM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #3

    Default

    I asked the same question a while back. 2% Lanthanated seemed to be a good all around. Sure some kinds of Tungsten seem to be a little better for one kind of welding but worse for others. Some people have a preference, it has to be this etc. Unless you are doing very specialized welding 2% lanthanated seems to be a good middle of the road.

    Thoriated was better for DC steel welding, but Lanthanted was pretty good. Just what I have picked up and I am not a TIG welder yet.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  4. #4

    Default

    2% Lanthanated is what i use all the time. I order some better welding tig gas lens today Click image for larger version. 

Name:	$(KGrHqZ,!qcE88ftTz9SBPerP2SJCw~~60_3.JPG 
Views:	693 
Size:	109.2 KB 
ID:	6972
    Last edited by Rodsmachineshop; 06-07-2012 at 05:39 PM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #5
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    2% Lanthanated is what i use all the time. I order some better welding tig gas lens today Click image for larger version. 

Name:	$(KGrHqZ,!qcE88ftTz9SBPerP2SJCw~~60_3.JPG 
Views:	693 
Size:	109.2 KB 
ID:	6972
    Hey Rod, where did you get your gas lenses? Or, where is a good place to pick up some good value gas lenses?
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  6. #6

    Default

    Quote Originally Posted by undercut View Post
    Hey Rod, where did you get your gas lenses? Or, where is a good place to pick up some good value gas lenses?
    Maybe river-weld.com ?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    Quote Originally Posted by undercut View Post
    Hey Rod, where did you get your gas lenses? Or, where is a good place to pick up some good value gas lenses?
    I saw the exact same package on E-bay ... don't rmrmber the vender but if you search tig consuables or tig torches it whould pull it up.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  8. #8

    Default

    Quote Originally Posted by undercut View Post
    Hey Rod, where did you get your gas lenses? Or, where is a good place to pick up some good value gas lenses?
    http://www.weldingcity.com/ $1.79 for wp-9 size and $2.79 for 17/18 size. I've made 3 orders there so far with no problems.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. #9

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    2% Lanthanated is what i use all the time. I order some better welding tig gas lens today Click image for larger version. 

Name:	$(KGrHqZ,!qcE88ftTz9SBPerP2SJCw~~60_3.JPG 
Views:	693 
Size:	109.2 KB 
ID:	6972
    I have been hobby TIG'n for at least 6 yrs, but just bought my first gas lens when I purchased the 250EX in March. I can not go without a gas lens now. I just recieved a large diameter gan lens...these things are massive.

    I was using zirconated for AC but I am trying those rare earth and have Lanthanated I have yet to try. I am digging my 250EX over the old Synchrowave 180 at this point. Love the 20WP torch, smaller and cooler.
    Millermatic 251 with 30A
    Synchrowave 180
    Hobart 100 MIG
    lathe & RF45
    Power TIG 250EX
    Spectrum 625 X-TREME
    Spray Zone.net-Side draft spray booth

  10. #10

    Default

    Quote Originally Posted by Winky View Post
    Been welding for about a decade but I am a noob when it comes to AC TIG welding ... in anticipation of the arrival of my new machine I stopped at Airgas yesterday grabbed some aluminum filler rod and asked the guy behind the counter for some 2% lanthinated tungsten ... he sees I have aluminum and tells me the lanthinated is for steel and stainless only ... I asked him what I should be using and he says pure tungsten. Now this guy has never steered me wrong before but I've heard from many people that pure tungsten is pure crap ... I think I even heard Jody say to stay with the 2% ... so now I'm totally confused.
    Winky, a good low price source for tungsten http://www.weldingcity.com/

    ken
    UNT 520D plasma/stick/tig; Hobart Handler 140 Mig; HF 80amp stick welder; Victor O/A; 4x6 Horizontal bandsaw; Planishing hammer; & Stuff

  11. #11

    Default

    Quote Originally Posted by KSmith View Post
    Winky, a good low price source for tungsten http://www.weldingcity.com/

    ken
    I will second that... I just picked up a couple sets from him. Best prices I could find...

    http://www.ebay.com/itm/200720864107...84.m1497.l2649

    http://www.ebay.com/itm/200720864107...84.m1497.l2649
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  12. #12

    Default

    I'll chime in here as well. As the prices seemed to good to be true.

    I have used his ER70 wire (what a deal I got on two spools back at Christmas $9 for 11lbs) and his 2% lanthanated for probably 6 months or more now. No problems at all. I like them much better than the weldcraft 2% thoriated I did use.

    His labeling looks cheap and made me nervous too when they showed. So far so good. I gave the weldcraft to a friend.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  13. #13

    Default

    Quick note. The new forum on shop tips and tricks, etc. Under chat lounge. If you want to get posts for any of the contest.

    Go there and talk about (review) the tungsten or a tool you made (Rod will win there). About to post up the plasma helper purchase now. Or a picture and general thoughts.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  14. #14

    Default

    Quote Originally Posted by KSmith View Post
    Winky, a good low price source for tungsten http://www.weldingcity.com/

    ken
    I placed an order with them 2 months ago. Order never went through. Emailed them and didn't hear nothing for a couple of weeks after that. Horrible service and I did not proceed with my order. I went to Weldfabulous and tried Weldcraft. I figured if weldcity had crap service then their products must be crap too, but that was just my experience with them.
    Millermatic 251 with 30A
    Synchrowave 180
    Hobart 100 MIG
    lathe & RF45
    Power TIG 250EX
    Spectrum 625 X-TREME
    Spray Zone.net-Side draft spray booth

  15. #15

    Default

    Quote Originally Posted by 5440 View Post
    I placed an order with them 2 months ago. Order never went through. Emailed them and didn't hear nothing for a couple of weeks after that.
    I see their ebay prices are higher... ehh... About .50 higher on a 10 pack. Not bad. I ordered through ebay and got them fast. Maybe they take care of ebay customers better... Feedback n all...
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  16. #16

    Default

    Quote Originally Posted by Brian Ski View Post
    I see their ebay prices are higher... ehh... About .50 higher on a 10 pack. Not bad. I ordered through ebay and got them fast. Maybe they take care of ebay customers better... Feedback n all...
    I've made three orders with them, all from their .com site, not ebay. I ordered a bunch of tig torch consumables first...they were out of stock on the tungsten I wanted. Then the tungsten came in, and I ordered that and some gas lens stuff. Finally, I ordered more tungsten and a flex head WP17 torch body. All came quickly, no problems. One time I was going to order, and they had a glitch in their shopping cart, but the next day it was fixed.

    ken
    UNT 520D plasma/stick/tig; Hobart Handler 140 Mig; HF 80amp stick welder; Victor O/A; 4x6 Horizontal bandsaw; Planishing hammer; & Stuff

  17. #17
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by KSmith View Post
    I've made three orders with them, all from their .com site, not ebay. I ordered a bunch of tig torch consumables first...they were out of stock on the tungsten I wanted. Then the tungsten came in, and I ordered that and some gas lens stuff. Finally, I ordered more tungsten and a flex head WP17 torch body. All came quickly, no problems. One time I was going to order, and they had a glitch in their shopping cart, but the next day it was fixed.

    ken
    I had good luck with the website too. Got gas lenses, torch parts, a pack of tungstens and a stick holder. They only had 1.5% when I ordered, but other than that, they shipped fast and everything seems to be decent quality.

    The one difference I've noticed about the lanthanated is that it seems to start much easier, especially at lower amperages.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  18. #18

    Default

    Quote Originally Posted by 5440 View Post
    I placed an order with them 2 months ago. Order never went through. Emailed them and didn't hear nothing for a couple of weeks after that. Horrible service and I did not proceed with my order. I went to Weldfabulous and tried Weldcraft. I figured if weldcity had crap service then their products must be crap too, but that was just my experience with them.
    Oh yea, I did have a problem, got the email address from paypal and did it that way. I think they are a one or two person show. But the materials are fine. I was shorted an item but they sent a paypal credit when I emailed (ordered two and they sent only one; didn't really need two).

    But yes, problem with order and a little communication delay as there was a mistake on my order. Also, it came in 3 parts as well, two boxes one day and another on the following. But time of year, that was probably not them.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  19. #19

    Default

    I'm going to get a little off topic here ... I tried using a sanding drum to dress my tungsten and it just didn't work well so I'm going to buy a 6" grinding wheel and dedicate it for tungsten what I was wondering ... every time I put a new wheel on my grinders I have to dress them down because the are always not as true as I like them ... since you want to keep a dedicated wheel for tungsten ... how can you dress it down without contaminating it?
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  20. #20
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    It gets so messed up from the tungsten that you don't bother dressing it. Actually the groove makes it easier.

    Seriously though, I got one of those cheap diamond dressers which shouldn't contaminate. But I never really thought about it.

    Gotta try the "slap a diamond wheel on the side of your grinder trick". I'll have to see if I can get away with side guards off though.

Similar Threads

  1. Fish tank stand... metal and process choice
    By Trip59 in forum General Welding Questions
    Replies: 4
    Last Post: 08-17-2012, 07:28 PM
  2. Lens # choice?
    By Trip59 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 36
    Last Post: 06-06-2012, 06:30 PM
  3. Tungsten Question
    By SeanMurphy265 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 09-12-2011, 03:22 AM
  4. Tungsten
    By bigjoeinkg in forum General Welding Questions
    Replies: 5
    Last Post: 08-29-2011, 01:17 AM
  5. Tungsten Grinder
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 07-22-2011, 01:03 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments