Thanks guys for the super fast response,After doing some troubleshooting by switching to lift start I could only get a tiny arc and thats with the tungsten literally touching my work piece.It also seemed like the welder was arcing without pressing the foot pedal so I quickly turned off the unit by the power switch in the back,then it hit me why not un plug the foot pedal and connect the torch switch.....and boom problem solved!.The foot pedal was causing all the issues.