It sounds like you have HF but no main arc transfer. The arcing inside between the points is normal. If the point gap was knocked out of adjustment from shipping you would have no starting arc. Be sure to check your ground clamp, and dinse connector for the wire pulling out. Lack of ground would cause your symptoms. You can also try stick mode and lift start TIG to provide more information for troubleshooting. Also AC and DC modes.