    Quote Originally Posted by Winky View Post
    Very cool ... you will love it
    I loved it up until my second session of welding a couple beads and the welder just stop working,no joke.All that it is doing now is giving me a very weak and faint arc and nothing more.I will be calling the office tomorrow,this just sucks seeing that I waited over a month for this welder and it completely died in a couple hours.

  2. #62
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Quote Originally Posted by watercooler View Post
    I loved it up until my second session of welding a couple beads and the welder just stop working,no joke.All that it is doing now is giving me a very weak and faint arc and nothing more.I will be calling the office tomorrow,this just sucks seeing that I waited over a month for this welder and it completely died in a couple hours.
    Not an expert, but that sounds suspiciously familiar... isn't that the arc gap issue, like a 5 minute fix?
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  3. #63

    Default

    or ran out of argon . i had that happen last week forgot to turn my gas on lol no arc
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  4. Default

    Yes I can see the arc inside the machine,how do I fix it??? and what caused this in the first place?

  5. Default

    I have a full tank of organ that I just bought for this machine the flow meter still showing full.

  6. #66

    Default

    make sure your ground clamp is good contact
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  7. #67

    Default

    what your lpm flow
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  8. #68
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    It sounds like you have HF but no main arc transfer. The arcing inside between the points is normal. If the point gap was knocked out of adjustment from shipping you would have no starting arc. Be sure to check your ground clamp, and dinse connector for the wire pulling out. Lack of ground would cause your symptoms. You can also try stick mode and lift start TIG to provide more information for troubleshooting. Also AC and DC modes.
    Long arc, short arc, heliarc and in-the-dark!

  9. Default

    Quote Originally Posted by Rodsmachineshop View Post
    what your lpm flow
    Its 7 lpm = 15 cfh and ground is good.

  10. #70

    Default

    are you using the peddle if so try with out and see if it works
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  11. #71

    Default

    also bad connection at power plug for the 220
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  12. Default

    Quote Originally Posted by Rambozo View Post
    It sounds like you have HF but no main arc transfer. The arcing inside between the points is normal. If the point gap was knocked out of adjustment from shipping you would have no starting arc. Be sure to check your ground clamp, and dinse connector for the wire pulling out. Lack of ground would cause your symptoms. You can also try stick mode and lift start TIG to provide more information for troubleshooting. Also AC and DC modes.
    Thanks guys for the super fast response,After doing some troubleshooting by switching to lift start I could only get a tiny arc and thats with the tungsten literally touching my work piece.It also seemed like the welder was arcing without pressing the foot pedal so I quickly turned off the unit by the power switch in the back,then it hit me why not un plug the foot pedal and connect the torch switch.....and boom problem solved!.The foot pedal was causing all the issues.

  13. #73

    Default

    lol i knew it lol darn foot peddles check and see if the pot took a crap or cog scipped in foot pedal
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  14. #74
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Nice to hear it was something easily replaced. Based on some people's pics of lack of strain relief on the pedal wiring. If it's okay with Oleg, and you feel like doing it, you might want to open the pedal and just see if a wire got pulled off. Could be easier to just fix it, than to send the pedal back for a replacement. And no down time waiting for shipping.
    Long arc, short arc, heliarc and in-the-dark!

  15. #75

    Default

    i called oleg to talk to him about the USA made peddle think i might buy one to review how well it works and how well its made
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  16. Default

    I can proudly say that my beads are now 100% better and no more arc wondering.That damn foot pedal was my problem all along now I am getting nice clean welds with out any weird arc wondering.I contacted Oleg on it so I am waiting on his response before I open it up.

  17. #77

    Default

    Quote Originally Posted by watercooler View Post
    Thanks guys for the super fast response,After doing some troubleshooting by switching to lift start I could only get a tiny arc and thats with the tungsten literally touching my work piece.It also seemed like the welder was arcing without pressing the foot pedal so I quickly turned off the unit by the power switch in the back,then it hit me why not un plug the foot pedal and connect the torch switch.....and boom problem solved!.The foot pedal was causing all the issues.
    By the time i got home , all was solved !
    Thanks to all who tried to help WaterCooler !
    Ray will call him and get the pedal issue fix
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  18. #78
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Oleg View Post
    By the time i got home , all was solved !
    Thanks to all who tried to help WaterCooler !
    Ray will call him and get the pedal issue fix
    Yeah, great bunch. I missed the whole episode - it was so short and so many people pitching in to help diagnose.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  19. Default

    Its nothing like having a product and great support to back it up.Update,I took the foot pedal at work to have our electronics tech diagnose and it appears to be the potentiometer is dead which seems like an easy fix.

Similar Threads

  1. Shipment is in !
    By Oleg in forum Everlast Announcements, Contests and Promotions
    Replies: 0
    Last Post: 07-11-2012, 03:26 AM
  2. UPS Shipment?
    By Gtig in forum Pre-sales, Sales and Shipping questions
    Replies: 5
    Last Post: 02-23-2012, 01:32 PM
  3. Next Shipment Due When`
    By bigjoeinkg in forum Everlast Announcements, Contests and Promotions
    Replies: 87
    Last Post: 08-11-2011, 01:50 PM
  4. The new shipment of 256's were said to look different....
    By ducksface in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 03-05-2011, 08:31 AM
  5. Update on new shipment ! Shipment is in.
    By Oleg in forum Everlast Announcements, Contests and Promotions
    Replies: 6
    Last Post: 07-21-2010, 09:52 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •