  1. Default Welding Nuts

    Anyone have any tips or tricks to welding nuts to pipe? I'm actually welding 1/4" nuts to 1/2" coupling nuts.

    Last time I put the bolt through the nut tacked and partially welded the nut and the bolt started sticking as the weld was cooling. Barely got it out and had to tap the nut to get another bolt in.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Quote Originally Posted by NRM View Post
    Anyone have any tips or tricks to welding nuts to pipe? I'm actually welding 1/4" nuts to 1/2" coupling nuts.

    Last time I put the bolt through the nut tacked and partially welded the nut and the bolt started sticking as the weld was cooling. Barely got it out and had to tap the nut to get another bolt in.
    For starters I would use square nuts. They have a lot more meat on them. Weld them on without a bolt in them and let them cool before putting the bolt in. TIG is the way to go and keep the arc focused on the thicker part and just wash the puddle up to the nut without putting too much heat into it. Also it helps to grind off any zinc plating before you start.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    After you weld the nut start running the bolt through the nut. Sometimes you still have to run a tap through the bolt because of distortion.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  4. #4

    Default

    Quote Originally Posted by NRM View Post
    Last time I put the bolt through the nut tacked and partially welded the nut and the bolt started sticking as the
    I thread the bolt through, usually just to align the nut with the hole drilled in the base metal. Then I back the bolt out while the nut is still hot and malleable. Seems to work with out needing to tap the nut again.

    Quote Originally Posted by Rambozo View Post
    TIG is the way to go and keep the arc focused on the thicker part and just wash the puddle up to the nut without putting too much heat into it.
    So, you did not use any filler? Just washed the base metal onto the nut? I may have to try that, as my welds came out really cold when I used filler. I probably had a hard time getting the heat focused because I was concentrating on jamming the filler in.

    Thanks
    Mike
    Power Pro 256

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Quote Originally Posted by posixPilot View Post
    So, you did not use any filler? Just washed the base metal onto the nut? I may have to try that, as my welds came out really cold when I used filler. I probably had a hard time getting the heat focused because I was concentrating on jamming the filler in.
    I usually use a little filler, but just get the puddle going good on the base metal before steering it towards the nut. Sometimes I use flange nuts, then you can just weld the flange and that's pretty easy, especially for sheet metal. It all depends on what kind of task you're asking of the nut. I'm a big fan of welding nuts onto items that get bolted together, so you can tighten the bolts with one tool. For that application I just need to keep the nut from turning, so a couple of deep tacks will do the job. If you are going to have more strain on the nut, you will prolly want a little more than that. However, if you weld two sides of a square nut, that will probably exceed the strength of the bolt, so welding all around is a bit of overkill. I don't usually have any problem in running a bolt in afterwards. 1/4" is a lil small, so keep a tight arc and watch the heat.
    Long arc, short arc, heliarc and in-the-dark!

  6. Default

    Thanks for the tips especially the square nut tip and I will be using SS nuts. I am going to see if I can get some if not I will use the standard nuts. I think I will use the bolt to line up the hole, tack it, remove the bolt and then finish the weld. I will use 1/16th tungsten and start the puddle on the coupling nut then flow the puddle into the nut. I’ll post pics of the outcome next weekend.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  7. Default

    Quote Originally Posted by NRM View Post
    Thanks for the tips especially the square nut tip and I will be using SS nuts. I am going to see if I can get some if not I will use the standard nuts. I think I will use the bolt to line up the hole, tack it, remove the bolt and then finish the weld. I will use 1/16th tungsten and start the puddle on the coupling nut then flow the puddle into the nut. I’ll post pics of the outcome next weekend.
    don't waste any time backing that bolt out.

  8. #8

    Default

    I did this on a jeep. I cut the old ones out and put some new ones back in. The first on I had to run a tap through it, and the second worked perfect. The second nut I turned the bolt up and down several times while it cooled down.


    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

Similar Threads

  1. Help! My 200DX went nuts!
    By rake in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 04-15-2016, 01:09 AM
  2. New cart design, am I nuts?
    By Trip59 in forum Other Custom Fabrications
    Replies: 15
    Last Post: 08-03-2012, 03:24 AM
  3. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •