One issue with with square nuts is that they are generally softer than even a grade 5 and have a grade 2 rating. Even though welding a nut removes some of the strength, it doesn't completely destroy the quality, and hardened nuts are welded all the time in the industry for this type application...Unless you can verify the hardness of the square nut, I wouldn't use it for welding.