    One issue with with square nuts is that they are generally softer than even a grade 5 and have a grade 2 rating. Even though welding a nut removes some of the strength, it doesn't completely destroy the quality, and hardened nuts are welded all the time in the industry for this type application...Unless you can verify the hardness of the square nut, I wouldn't use it for welding.

  2. #22
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Rambozo View Post
    Makes me want a TIG setup .... Any chance of me being successful at tacking a nut using a stick welder and a thin, fast freeze electrode? Can't try at the moment.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  3. #23

    Default

    Quote Originally Posted by undercut View Post
    Makes me want a TIG setup .... Any chance of me being successful at tacking a nut using a stick welder and a thin, fast freeze electrode? Can't try at the moment.
    There's no reason one couldn't use stick to weld nuts to a surface. Well, I wouldn't want to try tacking #8's, but a 1/4" nut (7/16" wrench) can be tacked easily enough. On a nut that size I'd use 1/16" rod, or 5/64. Tack it opposite sides, work around, alternating sides. Lean towards the thicker of the two metals you are joining. No sarcasm intended really, but it's not rocket science (in tribute to an old friend, Ray Bradbury, who died at 91 yesterday).

    ken
    UNT 520D plasma/stick/tig; Hobart Handler 140 Mig; HF 80amp stick welder; Victor O/A; 4x6 Horizontal bandsaw; Planishing hammer; & Stuff

  4. #24
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by KSmith View Post
    (in tribute to an old friend, Ray Bradbury, who died at 91 yesterday).
    Ohhhh. I didn't even hear about that. After looking, I see that CNN has the news. Clueless yahoo and msn haven't been updated yet.

    Quote Originally Posted by KSmith View Post
    There's no reason one couldn't use stick to weld nuts to a surface.
    Wasn't sure if the higher amperage of stick would warp the nut too much or not. Thanks. I'll need to give it a try - have a few items where welding the nut in place would be useful. Probably better alternatives for me to use but hey, any chance to weld is good, right!
    Last edited by undercut; 06-06-2012 at 06:23 PM.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  5. Default

    Sean I really like my rage 2. I cut a lot of SS aso I got the 90 tooth blade and it cuts well.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  6. #26
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by performance View Post
    One issue with with square nuts is that they are generally softer than even a grade 5 and have a grade 2 rating. Even though welding a nut removes some of the strength, it doesn't completely destroy the quality, and hardened nuts are welded all the time in the industry for this type application...Unless you can verify the hardness of the square nut, I wouldn't use it for welding.
    My local bolt store has them in both grade 2 and grade 5, but not grade 8. However, I can get flange nuts in grade 8 if needed. It all depends on the application and the size as to what kind of fasteners you select. For some jobs 1/4"-20 grade 2 is fine, for other 4"-4 grade 8 is not enough!
    Long arc, short arc, heliarc and in-the-dark!

  7. #27

    Default

    A flange nut or even a jet nut might be worth trying. S/F.....Ken M
    Lincoln Power MIG 300
    Everlast 160STH
    Miller 225 Thunderbolt (sold it)
    Lincoln Squarewave 175 TIG(traded it for)
    Miller DEL 200 welder/genset
    Thermal Dynamics 1250XL plasma cutter
    Miller XMT300

  8. #28

    Default

    Quote Originally Posted by Rambozo View Post
    My local bolt store has them in both grade 2 and grade 5, but not grade 8. However, I can get flange nuts in grade 8 if needed. It all depends on the application and the size as to what kind of fasteners you select. For some jobs 1/4"-20 grade 2 is fine, for other 4"-4 grade 8 is not enough!
    Then you would want some L-9's.

  9. Default Nuts Welded

    Here are the clamps (10) I made that needed to have nuts welded onto the flat side of some coupling nuts. It was easier than I thought but I think I should have moved the puddle into the nut a little more. After using the supplied torch for this I REALLY want the CK 130.
    Click image for larger version. 

Name:	IMG_20120611_081031.jpg 
Views:	523 
Size:	124.7 KB 
ID:	7088Click image for larger version. 

Name:	IMG_20120611_081042.jpg 
Views:	451 
Size:	126.0 KB 
ID:	7089Click image for larger version. 

Name:	IMG_20120611_081100.jpg 
Views:	512 
Size:	118.0 KB 
ID:	7090Click image for larger version. 

Name:	IMG_20120611_081117.jpg 
Views:	494 
Size:	121.1 KB 
ID:	7091
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  10. #30

    Default

    Quote Originally Posted by Rambozo View Post
    The better question is; are there such things as finished ones?
    BTW cadmium has not been used on fasteners in many years, but the silver zinc that is used is also no good for welding either, grind it off.
    Just saw this. Cadmium is still around and in common use. Buy them all the time.

Similar Threads

  1. Help! My 200DX went nuts!
    By rake in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 04-15-2016, 01:09 AM
  2. New cart design, am I nuts?
    By Trip59 in forum Other Custom Fabrications
    Replies: 15
    Last Post: 08-03-2012, 03:24 AM
  3. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •