Interesting link describing the different tungsten grinding angles for different requirements.
http://www.arc-zone.com/pdf/GrindingTungsten.pdf
rivets
 Member
					
					
						Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 Optimal Tungsten Grinding Angle
 Optimal Tungsten Grinding Angle
		Interesting link describing the different tungsten grinding angles for different requirements.
http://www.arc-zone.com/pdf/GrindingTungsten.pdf
rivets
 New Member
					
					
						New Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		I'll go ahead and say I'm against the grinding diagram in section 2. I personally grind AWAY from the rotation of the wheel. If it grabs in the configuration shown, it will try to kick that tungsten back at you, possibly into your hand. There was a thread over at weldinbweb just a few days ago where a guy shot a tungsten through the palm of his hand, most likely from a similar thing.
Vice Grips
WD-40
Duct Tape
 Member
					
					
						Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		Who would even suggest to grind on the high sideIt's just common sense that it could be dangerous that way....
I try to gring in a straight line most of the time but there are times I just slap it on the side of the grinding wheel for a quick touch up.