    The two I posted have better capability to resist unthreading, as they're physically locked in. The construction is more sound than a piece of wire stuffed in the hole. Everything has it's proper application, helicoils are fine for some things, but I'd rather go a step further and not worry about it.

    Then again, rather than sert-ing my sportster cases I'm cutting out one side of the thread boss, welding it back up and re-drilling/tapping (eventually).
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  2. #22

    Default

    as long as you put lock tite on the heli coil it stays in . i put lock tite on the heli coil before installing then install a bolt with anti seize on it tighten to proper torque anti seize makes the lock tite not stick to bolt threads . at the machine shop i use ez locks since most the time i need blind hole threads http://www.ezlok.com/InsertsMetal/installVideo.html
    Last edited by Rodsmachineshop; 05-30-2012 at 01:11 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #23

    Default

    Quote Originally Posted by Trip59 View Post
    The helicoils work well. Better if it is not a bolt that is inserted and removed often. They have been around for a long time. I have ran across the timeserts. Looks like they are the new school way of replacing threads.

    Thanks for the candle idea will have to give it a shot next time. I have tried welding the nut in place. Mostly with bad results, but will keep trying. I know I will run across more froze bolts.

    One thing I have learned over time. If the bolt feels like it is going to break... stop and give it some help. Usually heat will help a lot. Once you break it, it gets a lot harder to get it out.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  4. #24

    Default

    i get some bolts that just wont come out and end up putting on my Bridgeport mill and drilling out . have something like this to drill made my own they work good http://www.brokenbolt.com/small-brok...actor-demo.php
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #25

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    i get some bolts that just wont come out and end up putting on my Bridgeport mill and drilling out . have something like this to drill made my own they work good http://www.brokenbolt.com/small-brok...actor-demo.php
    Looks like a neat idea... As long as you have a flat surface to mount it to.

    I see they don't have a price. I just made a post a while back about places having things for sale that are so high priced they won't even put a price on them. Like the motorcycle/car on the side of the road with a ph # and no price. Price is so high they are embarrassed to put it in writing.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  6. #26

    Default

    make your own i did out of some 1 inch pieces of steel and use steel bushing from the hard store to have drill bit fit tight in hole. I make a lot of my own tools at my shop. need a wrench to do carrier bearing preload on a 14 bolt gm rear end wrench was 140 buck made it myself only cost like 3 bucks me making it . cant believe that much fro this wrench Click image for larger version. 

Name:	F14240760.jpg 
Views:	412 
Size:	59.4 KB 
ID:	6908
    Last edited by Rodsmachineshop; 05-30-2012 at 02:22 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  7. #27
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    make your own i did out of some 1 inch pieces of steel and use steel bushing from the hard store to have drill bit fit tight in hole. I make a lot of my own tools at my shop. need a wrench to do carrier bearing preload on a 14 bolt gm rear end wrench was 140 buck made it myself only cost like 3 bucks me making it . cant believe that much fro this wrench Click image for larger version. 

Name:	F14240760.jpg 
Views:	412 
Size:	59.4 KB 
ID:	6908
    You know, Rod, you could probably write an entire book about all of the tools you have either created from scratch, improved upon, or replicated ....
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  8. #28

    Default

    I prefer the timesert over the helicoil but still use a lot of helicoils, as they're left over and usually more than good enough. S/F.....Ken M
    Lincoln Power MIG 300
    Everlast 160STH
    Miller 225 Thunderbolt (sold it)
    Lincoln Squarewave 175 TIG(traded it for)
    Miller DEL 200 welder/genset
    Thermal Dynamics 1250XL plasma cutter
    Miller XMT300

  9. #29

    Default

    If you don't break the little tab off the end of the helicoil you can be in big trouble. I've seen where someone forgot to do that and the bolt just spun in the hole. We had to weld a tab to the end of the bolt and break out ye old slide hammer and go to town.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  10. Default

    Quote Originally Posted by Rodsmachineshop View Post
    I get so many broken bolts and studs at my shop , that the joy of a machine shop , i do a lot of heli coiling
    try using extractalloy rods, their slick as hell. just put a nut over the hole stick the rod down to the stud that broke off and weld it up through the nut do a swirley over the top of the nut grab a wrench and back it out. the first time i used it it blew me away it dont bother the threads in the hole at all.dont remember who makes it.

  11. #31

    Default

    Hi-alloy extractor is one brand. Seem it would make the job easier, but has a cost. If this is a common event in the shop probably worth it. Or TIG/torch round stock and a nut on.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  12. #32

    Default

    I've done that a handful of times with a 3/32 6011. it works on 3/8" and larger bolts.
    McGuire Irvine
    Crow Motor Co.

    Lincoln powermig 225 (work)

Similar Threads

  1. HF Ground Bolt?
    By Jacobelps in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 09-08-2016, 04:38 PM
  2. Steering 14 Bolt
    By GFab70 in forum Off Road Fabrication
    Replies: 0
    Last Post: 12-04-2015, 03:50 PM
  3. Need to find a bolt....
    By CGCINC in forum General Welding Questions
    Replies: 12
    Last Post: 10-17-2012, 01:57 AM
  4. EGR Valve Removal (jakeru's #15)
    By jakeru in forum On Road Fabrication
    Replies: 0
    Last Post: 07-20-2011, 06:52 PM
  5. TIG contamination removal techniques
    By jakeru in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 01-18-2010, 07:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •