Share
Results 1 to 7 of 7

Thread: PowerTIG DX200 DC works awesome! A/C mode blew up my Gas-lens!

  1. Default PowerTIG DX200 DC works awesome! A/C mode blew up my Gas-lens!

    SO I took a whack at TIG'ing some 1/4" Aluminum plate for the first time.

    I have been using the pedal and it's "Your guess is a good as mine" amperage setting.

    I had the pedal at about half way and the initial puddle was pretty good, but slow to form.

    I turned the pot up to 75% Amps, and struck the arc.

    A small poof happened and before I knew it, my Gas lens screens had been melted from a Piece of the tungsten (Red band) that has blown up.

    Why did this happen? Too much Argon? 1/16" Tungsten too thin? A/C frequency and balance off?

    Thanks for the help guys! Here is a shot of the exhaust I had made on DC mode.

    Click image for larger version. 

Name:	542063_10151734470055316_848165315_23820660_780514496_n.jpg 
Views:	560 
Size:	72.2 KB 
ID:	6878
    Spec-C Tuning and Fabrication

  2. #2

    Default

    1/4 inch aluminum should use 3/32 or larger . what do you have your argon set at and ac balance to high will do that .frequency 100hz or greater) gray band tungsten will allow you to weld aluminum with pointed tungsten. I myself usually just use a 1/8 for most stuff with a good point
    Last edited by Rodsmachineshop; 05-27-2012 at 05:49 PM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #3
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I think the 1/16" tungsten would be adequate if other parameters allowed it. Specifically: a low EP% AC Balance. Other important parameters for tungsten size selection: mixing in some Helium (allows smaller tungsten than pure argon), type of tungsten (2% lanthanated tungsten has highest current carrying capacity for its size).

    I would expect things to happen like a burning collet body (and other torch components incluidng melting the cup) only if you forgot to turn your gas on and lit a high-amp arc. Although you might see something like that happen if you used the wrong gas as well (like something that has reactive components in it, like a CO2 gas mix.)

    Hope this helps. PS - that stainless welds looks decent. I'm thinking making that stainless weld wouldn't have been possible without good purity gas.

    If needbe, for further diagnosis, post pics of your blown up torch parts, and torch shown setup the way you are using it.
    Last edited by jakeru; 05-27-2012 at 06:56 PM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  4. #4

    Default

    ac balance to high will fry things fast lol i have forgot to turn gas on when tigging woosh fryed lol
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #5

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    ac balance to high will fry things fast lol i have forgot to turn gas on when tigging woosh fryed lol
    Getting a short piece of 1/16 stainless filler mixed with your tungsten when grinding will get your heart going... when you light up with it as an electrode. I learned my lesson.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. Default

    Quote Originally Posted by zoama585 View Post
    Getting a short piece of 1/16 stainless filler mixed with your tungsten when grinding will get your heart going... when you light up with it as an electrode. I learned my lesson.

    LOL. Good to know I am not the only one that has done that trick. My buddy said he had never seen a big boy like myself jump up that quick.
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  7. Default

    Quote Originally Posted by zoama585 View Post
    Getting a short piece of 1/16 stainless filler mixed with your tungsten when grinding will get your heart going... when you light up with it as an electrode. I learned my lesson.
    Useless without pics!

    lol
    New to welding!
    Lots of Snap-On tools
    In need of more toys

Similar Threads

  1. Looking for stolen Powertig DX200
    By Snowdaze in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 07-30-2015, 11:41 PM
  2. Powertig 225 LX display erratic in pulse mode
    By Aaron in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 08-07-2013, 01:18 PM
  3. Question re: operation of pulse mode on PowerTig 200DX
    By Tantalum711 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 07-08-2011, 10:21 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •