If you ever bought a reground crankshaft and wondered what the stuff on the crank is it crankshaft grinding coolant we use that so cranks wont rust after regrinding . same stuff on new brake rotors and drums also .
If you ever bought a reground crankshaft and wondered what the stuff on the crank is it crankshaft grinding coolant we use that so cranks wont rust after regrinding . same stuff on new brake rotors and drums also .
EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list