hey see its getting rusty i use crankshaft grinding coolant to spray on metal will protect it from rusting and washes off with soap and water . i use a pump bug spayer to spray it , it mixes 20 to 1 so a gallon go along way http://www.cylinderheadsupply.com/cacrgrco1ga.html