Quote Originally Posted by undercut View Post
I believe both the online description and the manuals say that the blue flame variety supports TIG. Can anyone support this claim?
Depending on where you look you can find claims that is fine for TIG as well as warnings about it not being ok for low amperage TIG. I have a couple of them and the manuals change from time to time. They are not bad. I think the red one and the blue flame are the same guts, while the plainer one seems different. No comment on the skull. As long as you don't block the sensors they respond well to TIG. But they are only dual sensor, so it's possible to block them if you are welding around obstructions. Even if an autodark goes off from something, you might get dazzled but you shouldn't get a flash burn. They default to shade #4 when off and have full IR and UV filtering all the time.