The consensus seems to be that it's better to use a gas lens with a ceramic cup and extend the tungsten for better reach and visibility when need be.
The consensus seems to be that it's better to use a gas lens with a ceramic cup and extend the tungsten for better reach and visibility when need be.
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw