Share
Results 1 to 17 of 17

Thread: propane acetylene oxygen

  1. #1

    Default propane acetylene oxygen

    went over to a customer of mine she is a jewelry store owner and dose custom stuff tried her torch wow what difference with propane and oxygen when brazing and soldering , ask her why propane she said cooler and less contamination doing gold and silver
    Last edited by Rodsmachineshop; 05-17-2012 at 03:41 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  2. #2

    Default

    Rod, propane is way cooler in temp than acetylene...It won't be as hot no matter what you try.

  3. #3

    Default

    your rite i made boo boo lol dont know now maby she was rite by saying hotter read this http://www.cousesteel.com/AndysPlace...Acetylene.html it seamed a lot hotter to me when using her small torch BTU's of Acetylene is approximately 1470 btu's per cubic foot.
    BTU's of Propane is approximately 2498 btu's per cubic foot.
    Last edited by Rodsmachineshop; 05-17-2012 at 03:46 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  4. #4

    Default

    when i worked at a wreck yard we used propane to cut since cut faster and hotter so say the wrecking yard owner we thought he was cheap and didnt want to pay for more pricy gas lol
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #5

    Default

    Propane cuts slower and the flame is much cooler, so much that it is not able to gas weld. You use more oxygen as well.

  6. #6

    Default

    Click image for larger version. 

Name:	pACE3-6287926dt.jpg 
Views:	678 
Size:	81.2 KB 
ID:	6675with the rite tip it cuts good and fast , have to use a propane cutting tip not a standard tip . worked good at the wrecking yard must be he had the torches fit with propane tips
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  7. #7

    Default

    I've cut with propane, and have the tips...It requires a longer preheat time than OA as well.

  8. #8

    Default

    I tried that once... Since Propane is cheaper than acetylene. I got the right tip... Still have it somewhere. Usually the junk yards use propane because it is cheaper. Propane is a lot cheaper per tank, but propane does not seem to last as long. Usually I would go through 2 grill tanks for 1 acetylene. So if you use a lot it would benefit you. It didn't take more than a couple tanks to have me switch back. It didn't seem worth the trouble. IIRC the tips were more expensive and harder to find. I think I may have had to order one in. I think it was a 2 piece tip.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  9. #9
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Once the cut is started, the fuel is irrelevant and can even be turned off. It is the oxygen that does the real cutting. Try it sometime.
    Long arc, short arc, heliarc and in-the-dark!

  10. #10

    Default

    Quote Originally Posted by Rambozo View Post
    Once the cut is started, the fuel is irrelevant and can even be turned off. It is the oxygen that does the real cutting. Try it sometime.
    I've finished lots of cuts on steel after the acetylene ran out. Once that happens it helps to angle the torch toward the cut on thinner metal to get some preheat that the fuel would've provided when cutting normally.
    Last edited by zoama; 05-18-2012 at 02:04 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  11. #11

    Default

    I too use propane with my victor torch. I haven't used either gas enough to figure out which one is cheaper or cuts quicker, but I do like the fact that propane is cheaper and much easier to get if you happen to run out. As long as I set the flame right, I cant tell much of a difference between the 2 gases. I usually use a #1 propane/CNG tip for cutting 3/4 inch plate. It cuts through it like butter. Also, I like to use an oxidizing preheat flame because it seems to start much faster. the only down side is that the tip will get hotter.

    I have also used propylene and really liked it. It burns a bit hotter than propane, but is way too expensive to use.

    The thing I hate about propane is that its a bit harder to light when its windy and you cant light it with hot metal like you can with acetylene.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  12. #12

    Default

    i use a propane set up in a wrecking yard but mostly to cut sheet metal thin stuff sorta took along time to get thick stuff hot before cutting
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  13. #13

    Default

    When I was working in structural steel (earlys 2000's) this was a debate because of the cost of acetylene. The benefits were having your shop plumbed for propane which saved time. I think I went through one bottle of acetylene every one to two days. One to two bottles of oxygen a day (depending on how busy). A welder would run through one to two bottles of argon a day (depending on how busy). You loose 15-25 minutes changing out bottles. By the time you unhook everything, round up a dolly, and haul your bottles all the way across the shop; the company would loose a significant amount of time. Some companies were looking hard into plumbing their plants to save money and lost time. The main benefit is that just about every town has a propane company or at least one close by.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  14. #14

    Default

    Something else I remember... If you use Propane you have to use a special hose. It had to be rated for alternative fuels. Standard oxy acetylene hose was not rated to use propane. I check with my LWS and they stocked both hoses. Just the alternative fuel hose IIRC was more expensive. You could still use it with acetylene but not the other way around.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  15. #15

    Default

    Anyone ever try Oxy-Gasoline ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  16. #16

    Default

    thats cool
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  17. #17

    Default

    Quote Originally Posted by zoama585 View Post
    Anyone ever try Oxy-Gasoline ?
    All the fire dept special response teams typically use petrogen torches. They can get gas at any gas station and oxygen out of the ambulances and firetrucks. We're talking major structural collapse type stuff.

    We use oxygen and acetylene torches for working major truck crashes, and have a couple extra tanks on the major incident truck. Most of our cutting is done with gas chop saws: truck frames, springs, axles, etc.

    FWIW. S/F.....Ken M
    Lincoln Power MIG 300
    Everlast 160STH
    Miller 225 Thunderbolt (sold it)
    Lincoln Squarewave 175 TIG(traded it for)
    Miller DEL 200 welder/genset
    Thermal Dynamics 1250XL plasma cutter
    Miller XMT300

Similar Threads

  1. Cold Weather Power Equipment Starting Fluid on Steroids: Propane!
    By fyidiy in forum Personal Projects (no welder required)
    Replies: 0
    Last Post: 09-03-2018, 04:26 PM
  2. plasma or oxy acetylene
    By bobwills in forum General Welding Questions
    Replies: 15
    Last Post: 06-15-2012, 10:19 PM
  3. Buying oxy acetylene torch kit
    By bobwills in forum General Welding Questions
    Replies: 30
    Last Post: 05-10-2012, 02:13 PM
  4. What is 95/5 Argon/Oxygen gas used for???
    By Brian Ski in forum General Welding Questions
    Replies: 2
    Last Post: 03-22-2012, 05:01 PM
  5. Tell us about your OXY/ACETYLENE setup!
    By hooda in forum General Welder Questions
    Replies: 6
    Last Post: 05-02-2011, 09:48 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •