Thread: Dialing in my IMIG 200... Question?

  1. #1

    Default Dialing in my IMIG 200... Question?

    I cannot get the sizzle sound to be continuous. The wire will ball up on the end slightly until it burns off then it continues on, it's not bad because I've been adjusting everything and got it very close.
    I've adjusted the tension on the wire spool, tension on the rollers, wire feed speed/voltage but I just can't make it totally go away. The gas is a 75/25 mix of Argon/Co2 running at 20cfm(adjusted from 10 to 30 with no change). My nozzle is clean and I've tried many different angles.

    Is this normal or what am I doing wrong?
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    A good gound clamp is a must for a mig machine,,
    Some of those lies people tell about me, are true

  3. #3

    Default

    Quote Originally Posted by geezer View Post
    A good gound clamp is a must for a mig machine,,
    So the one supplied from the factory needs replaced?
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  4. #4

    Default

    Quote Originally Posted by CGCINC View Post
    So the one supplied from the factory needs replaced?
    The clamps supplied as original equipment are entry level to keep unit cost down,,,buying a better clamp will pay off in the long run,,especially on mig machine where contact is broken and restarted over and over in the process of wire feed
    Some of those lies people tell about me, are true

  5. #5

    Default

    I will do that! I don't think that is the cause of my issues I'm having right now though
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  6. #6

    Default

    yes clamp is cheesy i am getting a better ground clamp and also making the lead longer and heavier gauge . the ark force knob adjust wire stand out when in mig mode . took me awhile to get use to my 205 mig since my Lincoln mig is different
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  7. #7

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    yes clamp is cheesy i am getting a better ground clamp and also making the lead longer and heavier gauge . the ark force knob adjust wire stand out when in mig mode . took me awhile to get use to my 205 mig since my Lincoln mig is different
    Hmmmm... I DIDN't adjust Arc force because I thought that was only for Stick mode. Let me go try That!! Thanks
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  8. #8

    Default

    This is the one I use on my welders,,hard to beat it,,,,a good clamp,,,,http://store.weldingdepot.com/cgi/we...ot/GCTxxx.html
    Some of those lies people tell about me, are true

  9. #9

    Default

    arc force is to fine tune when you stop welding how much of your wire is sticking out when stopped ,Arc Force Control. This feature allows you to change arc qualities. When used in MIG mode, it helps to control wire burn back and stick out. These two factors help in start/stopping activities such as spot welding. When used in Stick/MMA/ SMAW mode, increasing or decreasing the “dig” can make the arc crisp and sharp or soft and buttery. This is helpful for making quality welds in and out of position. Some experimentation may be required to deter-mine the best setting for individual tastes from manual -- manual pdf http://www.everlastgenerators.com/downloads/mig.pdf lol i always read the manuals if on line before i even get my welders or buy the welder
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  10. #10

    Default

    Quote Originally Posted by geezer View Post
    This is the one I use on my welders,,hard to beat it,,,,a good clamp,,,,http://store.weldingdepot.com/cgi/we...ot/GCTxxx.html
    I just called the LWS and they have one so it's mine right after work!


    I think I have this thing dialed in now. I couldn't tell a difference with Arc Force in any position but after reading "Rods" post I guess I need to pay attention After I'm done welding. I gotta learn to read man U-L's..
    I was welding and I just kept thinking it seems like the spool is jerking as it is pulled into the torch. So I would pull the trigger and it rolled smooth!?!? Finally, instead of loosening the wing nut for the spool, I tightened it to within a half turn of tight and now it wizzes along perfectly and welds Awesome!! Of course I need more practice but with my new helmet I can now see what I'm welding so I'm ready to take on the world!!

    So just practicing, I welded this Stainless round bar to the mild 1/8" flat stock with the wire thats on the spool, E70s2. Would something like that hold?





    How would you stop burning the corner if you were to weld all the way around like this?
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  11. #11

    Default

    Quote Originally Posted by CGCINC View Post
    I just called the LWS and they have one so it's mine right after work!


    I think I have this thing dialed in now. I couldn't tell a difference with Arc Force in any position but after reading "Rods" post I guess I need to pay attention After I'm done welding. I gotta learn to read man U-L's..
    I was welding and I just kept thinking it seems like the spool is jerking as it is pulled into the torch. So I would pull the trigger and it rolled smooth!?!? Finally, instead of loosening the wing nut for the spool, I tightened it to within a half turn of tight and now it wizzes along perfectly and welds Awesome!! Of course I need more practice but with my new helmet I can now see what I'm welding so I'm ready to take on the world!!

    So just practicing, I welded this Stainless round bar to the mild 1/8" flat stock with the wire thats on the spool, E70s2. Would something like that hold?





    How would you stop burning the corner if you were to weld all the way around like this?
    Those are nice looking welds,,,it seems you have mastered mig,,,,wish I could be as consistant as those welds...nice work
    Some of those lies people tell about me, are true

  12. #12

    Default

    Quote Originally Posted by geezer View Post
    Those are nice looking welds,,,it seems you have mastered mig,,,,wish I could be as consistant as those welds...nice work
    Don't know about all that but getting a new helmet helped out Tremendously!!

    Now that it seems to be working properly, I have a lot more BB's than before.....
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  13. #13

    Default

    How far are you letting the wire get from the nozzle when you are welding?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  14. #14

    Default

    i have about 1/4 or so . get bb also but think it just my gas seems overtime i get anew bottle it welds better or worse know its the gas . also old mig wire will do that too
    Last edited by Rodsmachineshop; 05-15-2012 at 12:50 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  15. #15

    Default

    welds look good great deep penetration when i weld i start from each end and work inward then you dont get that melt away at end i do some short beads in center to stop warp oh what do you have your shielding gas flow set at i have my set about 10 seams to weld cleaner also what size wire spool size are you using and make sure the roll turn free and not binding and make sure you have the rite groove to drive the wire on the drive roller. also you will get bb if to high on amps since it gets into spray mode . were it melt before getting to surface your welding check this out https://docs.google.com/viewer?a=v&q...L4M1RzJx1vBiiw
    Last edited by Rodsmachineshop; 05-15-2012 at 01:07 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  16. #16

    Default

    It looks like he's running the wire out too far. I run my gas at 15 or 18 I can't remember. If your running crappy wire that could be some of the problem. Welding stainless to steel is probably some of your issue.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  17. #17

    Default

    yey sorta play with gas flow to see how it welds . Welding stainless to steel is probably some of your issue. i agree has to weld strange sorta like welding aluminized exhaust tubing lol
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  18. #18

    Default

    also what size wire .030 or .035
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  19. #19

    Default

    I notice more bb's when I let my arc length get too large, ie, less shielding, nozzle too far from the work. Your beads look great in my opinion.

    ken
    UNT 520D plasma/stick/tig; Hobart Handler 140 Mig; HF 80amp stick welder; Victor O/A; 4x6 Horizontal bandsaw; Planishing hammer; & Stuff

  20. #20

    Default

    I am running the gas at 20. I try to keep the nozzle as close to the work as I can butI'm sure it's probably farther than it should be, I would guess it at 1/2" or so sticking out.
    The wire size in it now is .030 but that's just about gone and I will be changing to an 11lb. roll of .035.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Similar Threads

  1. Power iMIG 275P Wire Feeder Alignment Question
    By Baronsbest in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 05-22-2016, 05:01 PM
  2. Help dialing in MIG on MTS 200
    By Jerry J in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 09-25-2014, 12:51 PM
  3. Dialing in the Imig 205
    By geezer in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 16
    Last Post: 12-28-2012, 10:48 PM
  4. Help dialing in your IMIG-205 welder (by Geezer).
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 0
    Last Post: 12-09-2011, 11:01 AM
  5. Imig 200 Question
    By SeanMurphy265 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 1
    Last Post: 08-01-2011, 01:16 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •