Share
Results 1 to 20 of 20

Thread: Anybody cutting 1"?

Threaded View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Anybody cutting 1"?

    I gave it a try and didn't do so good. I usually keep it at about 60# air, upped it to 70 for this and gave it full 70a. power. Cuts on the right don't count, I forgot to lower my lens shade down and was pretty much blind. Cut on the left I could see, but it didn't like it. Sounded like it was switching on and off.. I'm going to try again on the cut offs when I get some time. Any suggestions?
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	ap1.jpg 
Views:	496 
Size:	130.4 KB 
ID:	6572  
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

Similar Threads

  1. Powerpro 164 Plasma Cutter intermittently not cutting through 0.400" thk SS.
    By gtty in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 8
    Last Post: 08-03-2014, 01:00 PM
  2. 1/2" Cutting troubles, asking for insight
    By LMironworks in forum Everlast Plasma Cutters (PAC)
    Replies: 9
    Last Post: 02-04-2014, 05:27 AM
  3. Cutting a 4" circle....
    By CGCINC in forum Everlast Plasma Cutters (PAC)
    Replies: 9
    Last Post: 07-18-2012, 07:18 PM
  4. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-01-2011, 11:56 PM
  5. Oxy-Acetylene Cutting 1/2" Thick Steel Fire Barrel
    By jakeru in forum Other Custom Fabrications
    Replies: 0
    Last Post: 03-04-2011, 10:20 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •