Here is something else I want to try. Not saying that it will fix anything, but I can't see it hurting anything either.
http://www.weldingtipsandtricks.com/...gas-dryer.html
Here is something else I want to try. Not saying that it will fix anything, but I can't see it hurting anything either.
http://www.weldingtipsandtricks.com/...gas-dryer.html
Everlast Powertig 200DX
Miller Synchrowave 200
Miller Dynasty 300 (Work Machine)
Hobart Handler 210MVP
HTP Microcut 30
Injected65 - I think I'd try and recess those screens behind the opening of the cup a comfortable amount, to help ensure that the arc won't go through the screen. If an arc goes through the screen, it could mess the screen up in the short blink of an eye.
'13 Everlast 255EXT
'07 Everlast Super200P
I will experiment around with the screen positions. Thankfully he gave me 5-6 extra screens of each size.