The manual does not say anything about temp of storage. I would say you are fine. Most electronics are good to 140. It did mention stay away from moisture... But you should be fine with that...
One thing to watch for the higher the ambient temp it would affect the cooling of the unit and shorten the duty cycle of the welder. But we probably don't want to be out there that much longer either!!!!!