I am trying to weld aluminum. Running @ 150 amps. 1/8 thick. 3/32 rod, 1/8 2 % thor tungsten.
Everytime, the electorde gets a ball at the end of it. Or it blows the tip off. What am I doing wrong?
I am trying to weld aluminum. Running @ 150 amps. 1/8 thick. 3/32 rod, 1/8 2 % thor tungsten.
Everytime, the electorde gets a ball at the end of it. Or it blows the tip off. What am I doing wrong?
Purple Fabricator 211i