  1. #21

    Default

    Quote Originally Posted by Buggy Chief View Post
    There is one. I know I saw it not too long ago...It had a manual actuating arm...seems like it was on another forum.
    I figured there had to be one out there somewhere ... it seemed like a natural ... Thanks, I'll look around.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  2. #22

    Default

    was you talking about this I made one last week worked not that great , but got a better thought on making it
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. Default

    Quote Originally Posted by Rodsmachineshop View Post
    was you talking about this I made one last week worked not that great , but got a better thought on making it
    Yes it was similar. The one I saw was a vertical component though. Same concept.

  4. #24

    Default

    I didn't like this since if you trace something it ended up traced backwards. I ordered the roller bearing and came up with abetter set up to trace and do straight cuts . i ordered a 100 bearings http://www.vxb.com/page/bearings/PROD/Kit7339
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #25

    Default

    Quote Originally Posted by Buggy Chief View Post
    Not a problem. Thanks for quality products!
    Bought all three myself today.

    The ripper I will get the money back in a couple days just splitting squared tubing.. Circles guide, just for fun, anyone want my plastic one I made (hahaha). Bought the stand off after a little thought, was gonna skip that, but the Everlast one makes a mess of the nozzle sometimes on the A81 torch. Will let you know how good DeWaynes guides work as well as the stand-off on the Trafimet A81.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #26
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    I didn't like this since if you trace something it ended up traced backwards. I ordered the roller bearing and came up with abetter set up to trace and do straight cuts . i ordered a 100 bearings http://www.vxb.com/page/bearings/PROD/Kit7339
    Once you've got everything worked out, would love to see some pictures!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  7. Default

    Quote Originally Posted by everlastsupport View Post
    Bought all three myself today.

    The ripper I will get the money back in a couple days just splitting squared tubing.. Circles guide, just for fun, anyone want my plastic one I made (hahaha). Bought the stand off after a little thought, was gonna skip that, but the Everlast one makes a mess of the nozzle sometimes on the A81 torch. Will let you know how good DeWaynes guides work as well as the stand-off on the Trafimet A81.
    Would be interested to hear your feedback. I love the machined quality and the ultra fine adjustments on mine. I too, bought all three and have used them and been pleased. The only thing is for the straight guide, you may have to buy longer aluminum 3/8 dowels. the ones that come with it are about 12 inches long. I needed to rip the 4x10 sheets of aluminum, so I bought a 6' 3/8 aluminum dowel and cut it in half, giving me 2 Three foot sections. Good luck !

  8. #28

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    I didn't like this since if you trace something it ended up traced backwards. I ordered the roller bearing and came up with abetter set up to trace and do straight cuts . i ordered a 100 bearings http://www.vxb.com/page/bearings/PROD/Kit7339
    I would really like to see how your set up does ... please post when you get it worked out
    Last edited by Winky; 05-30-2012 at 01:43 AM.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

Similar Threads

  1. plasma cut pp205
    By jimmy in forum General Welder Questions
    Replies: 1
    Last Post: 11-14-2012, 05:52 AM
  2. What to use to cut Diamond Plate sheets?
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 34
    Last Post: 03-11-2012, 07:10 AM
  3. Anodized Aluminum Diamond Plate
    By Buggy Chief in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 01-13-2012, 11:56 AM
  4. Aluminum diamond plate flooring, for a fishing boat (jakeru's #10)
    By jakeru in forum Other Custom Fabrications
    Replies: 5
    Last Post: 07-15-2011, 04:19 PM
  5. Diamond Plate TIG Cart
    By dave s in forum Other Custom Fabrications
    Replies: 15
    Last Post: 03-29-2011, 06:09 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •