Share
Results 1 to 20 of 40

Thread: Pretty impressed with my PowerTIG 200DX

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default

    I like the green! I am a member of MANY web forums and this is by far the easiest on the eyes. I'm interested in how you like the 200dx as I am also thinking of using my 25% off discount on that unit (maybe). But I guess that depends on if I actually get to 100 or not
    Last edited by lucky13; 05-14-2012 at 05:47 AM.
    Newbie welder with just a Campbell Flux Core 80 watt "hot glue" gun, for now........

  2. #2

    Default

    Quote Originally Posted by lucky13 View Post
    I like the green! I am a member of MANY web forums and this is by far the easiest on the eyes.
    I agree as well. But some people must have different temps or settings. I can read it just fine. As well, I like seeing green...
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. Default

    Quote Originally Posted by everlastsupport View Post
    I agree as well. But some people must have different temps or settings. I can read it just fine. As well, I like seeing green...
    Quote Originally Posted by lucky13 View Post
    I like the green! I am a member of MANY web forums and this is by far the easiest on the eyes. I'm interested in how you like the 200dx as I am also thinking of using my 25% off discount on that unit (maybe). But I guess that depends on if I actually get to 100 or not
    lol, it makes my eyes do weird things. After I look at it for a while and look away everything looks kind off--like I've been sitting in the sun too long.

    Black background w/white webpages do the same. Maybe I'm just weird

  4. #4
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by ncsugrad2006 View Post
    lol, it makes my eyes do weird things. After I look at it for a while and look away everything looks kind off--like I've been sitting in the sun too long.

    Black background w/white webpages do the same. Maybe I'm just weird
    That's pretty natural. After looking at one color for a long time, they eyes get a bit used to it and will seem to get less sensitive to it temporarily. That's why colors seem a bit off afterwards. Your eyes will pretty much filter out some green until your eyes adjust.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  5. #5

    Default

    Quote Originally Posted by everlastsupport View Post
    As well, I like seeing green...
    I like seeing green too... in my wallet.

    I don't think the forum colors are offensive, but it definitely takes a few minutes for my eyes to acclimate.
    "Engineering is the art of modelling materials we do not wholly understand, into shapes we cannot precisely analyze so as to withstand forces we cannot properly assess, in such a way that the public has no reason to suspect the extent of our ignorance."

    - Dr. AR Dykes

  6. #6

    Default

    The green is nice. Green being the color that the human eye is most sensitive to, the layout should be fine. S/F....Ken M
    Lincoln Power MIG 300
    Everlast 160STH
    Miller 225 Thunderbolt (sold it)
    Lincoln Squarewave 175 TIG(traded it for)
    Miller DEL 200 welder/genset
    Thermal Dynamics 1250XL plasma cutter
    Miller XMT300

  7. #7

    Default

    Any more updates on the 200dx? I have pretty much decided on getting one and would like to hear some more experiences with the welder
    Newbie welder with just a Campbell Flux Core 80 watt "hot glue" gun, for now........

  8. Default

    Quote Originally Posted by lucky13 View Post
    Any more updates on the 200dx? I have pretty much decided on getting one and would like to hear some more experiences with the welder
    Same here. As soon as the ol mean green is over. Lots of videos on te 250ex and pp256 but I can't find a whole heck of a lot on the 200dx. I'm especially interested in the new one!
    New to welding!
    Lots of Snap-On tools
    In need of more toys

  9. #9

    Default

    Quote Originally Posted by ncsugrad2006 View Post
    Same here. As soon as the ol mean green is over.
    I think Everlast is going to sell a lot of inventory after this promotion is over. lol
    "Engineering is the art of modelling materials we do not wholly understand, into shapes we cannot precisely analyze so as to withstand forces we cannot properly assess, in such a way that the public has no reason to suspect the extent of our ignorance."

    - Dr. AR Dykes

  10. #10

    Default

    Quote Originally Posted by everlastsupport View Post
    I agree as well. But some people must have different temps or settings. I can read it just fine. As well, I like seeing green...
    Attached is the style. Make sue you tick the overwrite earlier versions box.

    www.redstickmoto.com/225/styles/
    Purple Fabricator 211i

Similar Threads

  1. PowerTig 200dx question
    By AnimalMother in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-25-2016, 01:44 AM
  2. PowerTIG 200DX
    By Sparky_Mark in forum Pre-sales, Sales and Shipping questions
    Replies: 4
    Last Post: 10-18-2015, 04:09 AM
  3. powertig 200dx problem
    By babowtie in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 02-01-2015, 04:30 PM
  4. Buy the Powertig 200dx or save for The Dynasty 200dx
    By AfroPaul in forum TIG Welding (GTAW/GTAW-P)
    Replies: 40
    Last Post: 05-13-2013, 07:18 PM
  5. PowerTig 200DX Cover
    By earla in forum Other Custom Fabrications
    Replies: 2
    Last Post: 09-01-2011, 12:23 PM