There is a market for the V6 Camry/Solara guys, but no one seems to take heed of that.

So before I got my PowerTIG 200dx, I had a GiantCrap 3-in-1 that would only let me scratch start..

Here are some pictures of the process. I am positive the Everlast will do miles more then the other welder I had!

Before.

Click image for larger version. 

Name:	557767_10151442251915316_848165315_23048783_1613241663_n.jpg 
Views:	532 
Size:	106.9 KB 
ID:	6450
Click image for larger version. 

Name:	531030_10151442252300316_848165315_23048784_1065382333_n.jpg 
Views:	480 
Size:	92.4 KB 
ID:	6451

These are the holes that the air normally came in, crazy restriction!

Click image for larger version. 

Name:	485783_10151442252850316_848165315_23048789_1920430282_n.jpg 
Views:	517 
Size:	16.6 KB 
ID:	6452

Then tacking and fabbing.

Click image for larger version. 

Name:	562459_10151553959830316_848165315_23438466_728233368_n.jpg 
Views:	541 
Size:	77.4 KB 
ID:	6453
Click image for larger version. 

Name:	527967_10151553960155316_848165315_23438469_431232189_n.jpg 
Views:	533 
Size:	88.9 KB 
ID:	6454
Click image for larger version. 

Name:	578031_10151553960490316_848165315_23438473_936327553_n.jpg 
Views:	533 
Size:	64.1 KB 
ID:	6455
Click image for larger version. 

Name:	525968_10151553960845316_848165315_23438477_1851269763_n.jpg 
Views:	542 
Size:	94.0 KB 
ID:	6456

Then installed.
Click image for larger version. 

Name:	525879_10151442258530316_848165315_23048818_1892566255_n.jpg 
Views:	517 
Size:	93.7 KB 
ID:	6457
Click image for larger version. 

Name:	562653_10151442259410316_848165315_23048822_2057918445_n.jpg 
Views:	533 
Size:	78.7 KB 
ID:	6458
Click image for larger version. 

Name:	541326_10151442251525316_848165315_23048781_1713652101_n.jpg 
Views:	513 
Size:	65.3 KB 
ID:	6459


AFTER!


I hope to improve the quality with the new POWERTIG!