This is an Aluminum outdoor Sign frame for the top of my building.
I will be wrapping the 2' x 6' Aluminum .090 sheet with my sign wrap that is getting printed.
After checking on prices of Aluminum channel, I decided to make this with angle instead.
2" angle for the triangle supports and 1" angle for the sign frame. 1/8" material.
It's really pretty basic and my welds aren't perfect but for my purpose it should be just fine.
![]()