I would at least get the 185 micro if you want cheaper, then you have the option of going AC if you want. If you have a Tig you will want to weld Aluminum at some point, if not like Rod said a mig is much easier for sheet metal and thin stainless. All I ever used at the bodyshop for 25+ years was a mig, that was for any sheet meatal and frame welding we ever did.