  1. Default Recommended Settings?

    Is there a calculator or resource that has recommended settings based on metal on thickness that you desire to cut?

  2. #2

    Default

    No chart that I am aware of. There are a couple of things to keep in mind. One is the speed that you move, the other is our machines cut a little stronger than most I have used. So others chart will get you close and you might have to back it down a bit.

    I normally use 30-40 for 3/8" or less, and 60 (max) over 3/8". I move fast or use a straight edge when I can. But what works for me might not work for others. Old school was, I think, was 1 amp for every 1/100, but like I said our units tend to be a little hotter than most. You can try that though.

    The old rule was 50 amps for .5" and 75amp for .75" (3/4"), but if you take our Power Plasma 50, it will clearly cut up to 1" at 50amps and a little more.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. new 250ex settings
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 01-28-2015, 01:59 AM
  2. pulse settings
    By Winky in forum TIG Welding (GTAW/GTAW-P)
    Replies: 37
    Last Post: 07-07-2012, 02:14 PM
  3. Why is E6010 not recommended on the 225LX?
    By Paul Moir in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 05-26-2012, 11:15 PM
  4. EXT250 HF gap settings
    By todmorg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 12-23-2011, 03:09 AM
  5. ac tig settings
    By iil in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 12-24-2010, 01:46 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •